Author: Subject: Calamine--ZnCO3
darkflame89
Hazard to Others
***




Posts: 255
Registered: 1-3-2004
Location: With probability 1, "somewhere" in this
Member Is Offline

Mood: No Mood

[*] posted on 2-4-2004 at 01:53
Calamine--ZnCO3


Saw a bottle of calamine at my pharmacy. I checked up my books and they said it was ZnCO3. I need to obtain it pure but the bottle contains menthol too. Anyway to get rid off it??

Incidentally, is there anyway to recover zinc metal from zinc carbonate?




Ignis ubique latet, naturam amplectitur omnem.
View user's profile View All Posts By User
I am a fish
undersea enforcer
****




Posts: 600
Registered: 16-1-2003
Location: Bath, United Kingdom
Member Is Offline

Mood: Ichthyoidal

[*] posted on 2-4-2004 at 02:21


In my experience, medicinal products are generally poor and expensive sources of laboratory chemicals.

Zinc oxide is cheaply and readily available from pottery suppliers. If you particularly want to make the carbonate:

1. Dissolve an excess of zinc oxide in sulphuric, hydrochloric or nitric acid.
2. Filter out the excess zinc oxide, to give a pure solution of the zinc salt corresponding to the acid used.
3. Add sodium carbonate solution, to precipitate out zinc carbonate.

A brief overview of methods to extract zinc from its compounds can be seen here:
http://www.webelements.com/webelements/scholar/elements/zinc...

A readily available source of zinc metal is the casing of zinc-carbon batteries.




1f `/0u (4|\\| |234d 7|-|15, `/0u |234||`/ |\\|33d 70 937 0u7 /\\/\\0|23.
View user's profile Visit user's homepage View All Posts By User
Organikum
resurrected
*****




Posts: 2339
Registered: 12-10-2002
Location: Europe
Member Is Offline

Mood: frustrated

[*] posted on 2-4-2004 at 02:38


zinc-oxide is even more readily available at paintstores - zinc-white as pigment for white paint.

For the rest see what the fish wrote - he is absolute right.




Irgendwas is ja immer
View user's profile View All Posts By User
darkflame89
Hazard to Others
***




Posts: 255
Registered: 1-3-2004
Location: With probability 1, "somewhere" in this
Member Is Offline

Mood: No Mood

[*] posted on 2-4-2004 at 02:41


Unfortunately, where i live do not have such luxury. But I see the point about zinc from batteries. Can i just peel of the outer layer and react with it?



Ignis ubique latet, naturam amplectitur omnem.
View user's profile View All Posts By User
Saerynide
National Hazard
****




Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline

Mood: Ionic

[*] posted on 2-4-2004 at 02:42


I thought the can on the Zn/C batteries was a zinc alloy?
View user's profile View All Posts By User
I am a fish
undersea enforcer
****




Posts: 600
Registered: 16-1-2003
Location: Bath, United Kingdom
Member Is Offline

Mood: Ichthyoidal

[*] posted on 2-4-2004 at 02:52


Technically yes, but the zinc content is usually over 99%.