[*] posted on 1-6-2009 at 19:45
preparation of uranium/uranyl sulfates


Can anybody suggest a process for the preparation of uranyl sulfate and/or uranium sulfate from the metal?
View user's profile View All Posts By User
not_important
International Hazard
*****




Posts: 3873
Registered: 21-7-2006
Member Is Offline

Mood: No Mood

[*] posted on 1-6-2009 at 22:02




Quote:
Sulfurlc acid-hydrogen peroxide mixtures react slowly with the metal. at 75°C forming uranyl sulfate.— The addition of small amounts of chloride or fluoride to H2S04 - H202 mixtures increases the dissolution rate.


From a LANL paper which referenced:
R. P. Larson, Anal. Chem. 31, 545 (1959)
Dissolution of Uranium Metal and its Alloys.

http://pubs.acs.org/doi/abs/10.1021/ac50164a026


Perhaps someone with full access can retrieve the Anal. Chem. paper for details.
View user's profile View All Posts By User
pantone159
National Hazard
****




Posts: 588
Registered: 27-6-2006
Location: Austin, TX, USA
Member Is Offline

Mood: desperate for shade

[*] posted on 2-6-2009 at 06:29


Paper attached.


Attachment: solution_u_metal_ac50164a026.pdf (701kB)
This file has been downloaded 996 times
View user's profile Visit user's homepage View All Posts By User
merrlin
Hazard to Others
***




Posts: 110
Registered: 3-4-2009
Member Is Offline

Mood: No Mood

[*] posted on 2-6-2009 at 10:10


@ not_important & pantone159,

Thanks for the abstract and paper. The processes described appear to be quite manageable.
View user's profile View All Posts By User
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 5-6-2009 at 03:58


I just posted the 138 page Chapter LXIII on Uranium from Volume XII of Mellor's "A Comprehensive Treatise on Inorganic and Theoretical Chemistry", it is in the New Books (Inorganic Chemistry) forum in References.

The section on uranium sulfates is attached.

[Edited on 5-6-2009 by Sauron]

Attachment: Pages from Uranium.pdf (569kB)
This file has been downloaded 979 times

[Edited on 5-6-2009 by Sauron]




Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
merrlin
Hazard to Others
***




Posts: 110
Registered: 3-4-2009
Member Is Offline

Mood: No Mood

[*] posted on 5-6-2009 at 11:12


@ Sauron,

Thanks for the excerpt. It is fascinating how much fundamental work from the past two centuries is out there in scanned literature that is apparently inaccessible by keyword searches. I will contact you regarding access to the References section.
View user's profile View All Posts By User
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 5-6-2009 at 15:34


You can't really expect keyword searches to do everything.

Just as regards Mellor's 16 volumes, until a few weeks ago, only volumes 1, 2, 8, amd half of 10 plus a lone chapter from 11 were scanned and on the Net at all, mostly through one of our members S.C. Wack. Then some damn fool (me) decided to scan the rest of it and I am pleased to say the end is near. Then there are 8 supplements to attack. But those are concerned only with the halogens, alkali metals, N, P and B.




Sic gorgeamus a los subjectatus nunc.