[*] posted on 2-4-2009 at 13:47
Preparation of Sodium Aluminum Hydride and Lithium Aluminum Hydride


In another thread zed complained that the prep of LAH many of us have seen on Rhodium is not very satisfactory because it is wasteful of lithium hydride.

4 LiH + AlCl3 -> LiAlH4 + 3 LiCl

and the more I thought about it the more I decided she is right.

She suggested

Li + Al + 2 H2 -> LiAlH4

which is a heat/pressure reaction. She could not immediately recall the reference.

I was curious about just how much heat and pressure was involved and this led me to an Ethyl Corp patent by Ashby. It seems his process worked better for sodium aluminum hydride than for lithium, and anyway usually run at 5000 psig H2 pressure.

Furger paper chasing revealed an improvemnt assigned to same company by Nelson, which allowed pressures to be reduced to 1000 psig. Much more to my liking. Especially so since NaAlH4 reacts with LiCl to produce LiAlH4.

So now we have a two step process to prepare LAH from Na, Al, H2, and LiCl. No lithium hydride required.

The Ashby/Nelson process is done in toluene not Et2O or THF. A small amount of triethylaluminum is used as catalyst.

So at this point the problem becomes: how to obtain or prepare triethylaluminum?

This is simpler than it sounds.

Caution: trialkylaluminum compounds are usually spontaneously pyrophoric. Study up on Schlenk type manipulations under dry N2.

You can start with Al (turnings, granules, powder). It needs to be clean and dry and as oxide free as possible. This is reacted with ethyl chloride or better, ethyl bromide, adding the halide to the Al a little at a time because the reaction is exothermic and the halide volatile. A small amount of I2 is used to start things. Once the reaction subsides, add a little more halide. Repeat until complete. This is described in Brauser for diethylaluminum bromide.

The reaction between Al and 3 EtX produced what is referred to for convenience as ethylaluminum sesquihalide Et3AlX3. In fact there is no such beast. The sesquihalide is an rquilibrium mixture of EtAlC2 and Et2AlX. Unfortunately these cannot be fractionated. There are however workarounds.

Option 1: Reduce the dihalide to halide with an active metal alloyed with the Al in the original reaction. Mg is used in this case and the stoichiometry dictates a 70% Al 30 % Mg alloy called magnalium. This is what is used in Brauer.

Option 2: reduce the sesquihalide with Na metal after the fact.

Option 3: complex the EtAlCl2 with NaCl, now the distillation will work because the desired Et2AlCl2 does not complex with NaCl.

EtAlCl2 + NaCl -> Na(EtAl)Cl3 solid

I am awaiting the paper on this. I do not know if this works for sesquibromide and NaBr.

I am also unsure of whether the solid complex can be reduces with Na. But, Al and EtCl are cheap so why would it matter?

All of these are viable.

Once Et2AlX is in hand, it can be reduced with Na to Et3Al. The triethylaluminum is distilled off the NaX byproduct. It is best stored either neat or in a 25% w/w soln in toluebe and in a Sure/Pak type cylinder.

Zed calculated that the NaAlH4 prep in a 1 L autoclave like my Parr, will produce 225 g or so NaAlH4. About half a pound per run. A run like that requires only a few ml triethylaluminum and the solvent and catalyst can be reused several times without replenishment. So a little triethylaluminum goes a long way.

The papers I collected on these reactions are mostly in the Parr Shaker Hydrogenator thread and the Need Help From the Pyrotecnics Side thread. A few more I will post here.



[Edited on 2-4-2009 by Sauron]




Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 3-4-2009 at 00:37
From Ullmann's


2.3.2. Reaction of Aluminum With Alkyl Halides to Make Alkylaluminum Sesquichlorides

"Methyl, ethyl, and other alkyl or aralkyl halides that are not dehydrohalogenated readily, can react with aluminum metal in an exothermic process to form organoaluminum sesquihalides in high yields [38], [39]. An important example is the reaction of methyl chloride [74-87-3] with aluminum [7429-90-5].
3 CH3Cl + 2 Al -> (CH3)3Al2Cl3 (15)
The reaction is carried out with aluminum in the form of turnings, shavings, granules, or powder. Oxygen and moisture must be rigorously excluded. The reaction can be initiated with a small amount of mercury or iodine. It also can be started by treating the aluminum with an alkylaluminum halide. A portion of the residue from a previous reaction is effective.
The products are equilibrium mixtures of the codimer (R2AlX · RAlX2) and homodimers [(R2AlX)2 and (RAlX2)2], in which the two aluminum atoms of each component are halogen-bridged as shown by compound 3, Section 2.1. Physical Properties.
In the reaction of methyl chloride [74-87-3] with aluminum, small amounts of ethane are formed by an apparent Wurtz-like reaction. With ethyl chloride, some butane is produced; also, dehydrochlorination of ethyl chloride can occur to form byproduct ethylene and excess Al – Cl bonds in the product. The ethylene may form oligomers in the mixture by a cationic mechanism. The byproduct reactions are favored by higher temperatures and therefore can be minimized by careful temperature control. When byproduct reactions take place to a significant extent, the excess Al – Cl content in the R3Al2Cl3 product can be decreased by addition of the calculated amount of R3Al. Overall, however, it is critical to control reaction conditions as slight excursions can result in catastrophic events.
Products can be recovered by settling and decantation, filtration, or distillation. Large quantities of methyl- and ethylaluminum sesquichlorides are produced industrially by this method. They are used as alkylating agents, catalyst components, and for making other methyl- or ethylaluminum chlorides.
Process Example. Production of ethylaluminum sesquichloride by reaction of ethyl chloride with aluminum is illustrated by this patent example [39]. A 9.5 × 10–2 m3 closed steel reactor, fitted with a reflux condenser and equipped for vacuum distillation of product, was first purged with nitrogen. After addition of 13.6 kg of aluminum powder and a catalyst mixture composed of 3.6 kg diethylaluminum chloride and 410 g iodine [7553-56-2], the reactor contents were stirred and heated slowly to 130 °C. The temperature was maintained at 120 – 150 °C during addition of 50 kg ethyl chloride over a period of 3 h.
The product can be flash distilled under vacuum, or it can be drained from the reactor and clarified by settling or by filtration of black residual metal solids. Iodine can be omitted from the procedure, in which case the induction period may be increased.


2.3.3. Reduction of Alkylaluminum Sesquichlorides to Make Trialkylaluminums

The alkylaluminum sesquihalide products from aluminum reactions with alkyl halides can be converted to dialkylaluminum halide or trialkylaluminum materials by treatment with active metals, such as sodium [7440-23-5] or magnesium [7439-95-4] [38], [39]. For example, diethylaluminum chloride or triethylaluminum can be produced from ethylaluminum sesquichloride by sodium reduction.
2 (C2H5)3Al2Cl3 + 3 Na -> 3 (C2H5)2AlCl + Al + 3 NaCl (16)
3 (C2H5)2AlCl + 3 Na -> 2 (C2H5)3Al + Al + 3 NaCl (17)

A magnesium-aluminum alloy can provide the reduction function concurrently with reaction between aluminum and the alkyl halide.
The sesquichloride reduction process is currently the most economical route available for production of trimethylaluminum.
Trialkylaluminum products made by this process generally contain trace levels of residual chloride but do not contain Al – H or other low-level components found in the aluminum-hydrogen-olefin processes (Section 2.3.1. Hydroalumination to Produce Trialkylaluminums).
The components of ethylaluminum sesquichloride cannot be separated economically by fractional distillation because of unfavorable vapor pressure relationships. However, diethylaluminum chloride can be distilled from the crystalline sodium chloride complex that forms with ethylaluminum dichloride [22].
(C2H5)3Al2Cl3 + NaCl ® (C2H5)2AlCl + Na[Al(C2H5)Cl3 (19)
Process Example. Diethylaluminum chloride has been made industrially according to Equation 16. In a patent example [39], ethylaluminum sesquichloride (26.5 kg) added to a nitrogen-purged 9.5 × 10–2 m3 reactor, was heated to 175°C. Then, while the mixture was stirred vigorously, 1.1 kg sodium was added over a 30 min period; the mixture was further heated at 155 – 190°C for 60 min. The diethylaluminum chloride product distilled from the reactor at 100 – 161°C (1.3 – 6.1 kPa).
In this example, an excess of ethylaluminum sesquichloride was employed to facilitate draining the voluminous byproduct salt and aluminum solids from the reactor. In an alternate approach, a heavy hydrocarbon oil, added prior to reaction, may be employed to remove the solids in slurry form, permitting the use of a stoichiometric ratio of ethylaluminum sesquichloride and sodium reactants.

2.3.5. Reproportionation Reactions

When alkylaluminum halide or trialkylaluminum compounds and aluminum trihalides are combined, reproportionation reactions occur rapidly under ambient blending conditions, releasing small amounts of energy [38], [39]. These reactions are of industrial importance in making, e.g., diethylaluminum chloride or ethylaluminum dichloride. Either can be formed, depending upon reactants and stoichiometry chosen.
2 (C2H5)3Al + AlCl3 -> 3 (C2H5)2AlCl (21)
(C2H5)3Al + 2 AlCl3 -> 3 C2H5AlCl2 (22)
(C2H5)3Al2Cl3 + (C2H5)3Al -> 3 (C2H5)2AlCl (23)
(C2H5)2AlCl + AlCl3 -> 2 (C2H5)AlCl2 (24)
This method is particularly useful for making alkylaluminum halides that cannot be produced via the reactions of aluminum with alkyl halide, e.g., diisobutylaluminum chloride and isobutylaluminum dichloride. These are preferred over the corresponding ethyl homologues as co-catalysts in certain olefin polymerization systems."


I have emphasized the key sections on bold. Note that one mol of Et3Al will react with one mol of the "sesquichloride" Et3AlCl3 to give three mols Et2AlCl, which can then to reduced with Na to 2 mols Et3Al - a more efficient exploitation of the sesquichloride than other methods, (Eq 23)


[38] A. von Grosse, J. M. Mavity, J. Org. Chem. 5 (1940) 106 – 121.


[Edited on 3-4-2009 by Sauron]




Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 3-4-2009 at 23:09


The angels of References appear to be pulling a work slowdown, so that paper from Liebig's Annalen has not materialized. However no matter as I found this short and sweet note from the Ethyl Corp. in 1938 describing their prep of ethylaluminum sesquichloride and related compounds, and inclusing the separation of RAlX2 from R2AlX by complexing the former with NaCl.

This invovles adding an excess of NaCl, heating, and distilling the liquod diethylaluminum chloride from the solid complex. As the original mixture is almost exactly 1:1 this amounts to 50% based on the somewhat imaginary sesquihalide Et3AlCl3.

This is similar to the yield obtained by reduction of the sesquihalide with Na metal. But obviously NaCl is cheaper and easier to obtain than Na.

Interestingly they used by preference Alcoa #12 alloy which is 8% Cu but the Cu does not appear to react with the halide nor is it observed upon analis of the alkylaluminum products. I see no reason why c.p. Al will not work just as well.

Attachment: ja01276a504.pdf (83kB)
This file has been downloaded 783 times

[Edited on 4-4-2009 by Sauron]




Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 4-4-2009 at 07:28


Quote: Originally posted by Sauron  

Interestingly they used by preference Alcoa #12 alloy which is 8% Cu but the Cu does not appear to react with the halide nor is it observed upon analis of the alkylaluminum products. I see no reason why c.p. Al will not work just as well.
I can think of two possibilities:
* The alloy is more easily machinable into pieces of high surface area.
* The copper is catalytic. I noted that they add AlCl<sub>3</sub> or the product of a previous preparation. The copper chloride species are perhaps intermediates.

A point on semi-industrial manufacturing occurred to me. The byproduct EtAlCl<sub>2</sub>.NaCl might work as a raw ingredient to a subsequent batch. Since the raw ingredients are solid and gas with liquid products, the double salt byproduct will be in intimate contact with the co-solution of the two product species. Since the equilibrium of this solution is an equal partition, half of the byproduct should be converted as well. The upshot would be a sequential-batch process in which there would be a constant volume of byproduct at any given time.

The open question is whether the double salt dissolves or not. Even a relatively low solubility would be sufficient. Stirring might be required for an adequate reaction rate.
View user's profile View All Posts By User
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 4-4-2009 at 09:08


The closest common alloy is 2024 and even closer is 2019.

Anyway no other report on reaction of Al and alkyl halides makes such a claim. The most common catalyst is I2,

If "magnalium" 70% Al 30% Mg is available then no EtAlCl2 is isolated, as the Mg reduces it to Et2AlCl. In this case the use of the complex is not required nor possible.

Certainly it would be convenient to make use of the complex if possible. Perhaps it might be broken thermall.

And the other option if the Al/Mg is not available is to merely make the sesquihalide and convert it to a mol or two of Et2Al.

Thereafter, further sesquihalide is reacted with Et3Al to produce Et2AlCl thus exploiting the sesquihalide's two components in full.

Et3Al2Cl3 + Et3Al -> 3 Et2AlCl

So the complex is only involved in the first mol or two, and the "waste" in not ongoing thereafter.

Of course the Na reduction of diethylaluminum chloride is not quite mol for mol

3 Et2AlCl + 3 Na -> 2 Et3Al + Al + 3 NaCl





Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
zed
International Hazard
*****




Posts: 2281
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 5-4-2009 at 01:45


My beloved little grand daughter Munchkinkiss, has suggested to me that one might intimately wrap together a 70/30 mixture of fine Aluminum Wire with fine Magnesium wire, place a length of that wire in a vacuum, and then conduct the current from two wired in parallel 12 volt car batteries thorough it, thereby blowing it to molten smithereens. The beads of metal recovered might then approximate the composition of the required alloy.

I'm not sure she's right, but she might be. Such an arrangement is surely capable of quickly melting the metal without oxidation. As I recall, it will instantly explode 12 gauge copper wire into a brilliant flash of light and a dispersed collection of bright micro-BBs.

When you try this trick on copper, in the atmosphere, you get a hot copper wire.
When you do it in the perfect insulation of a vacuum; Shazzam! You get instant molten copper.

Personally, I hope there is a better way to get through that NaAlH4 synthesis.
Either via a catalyst other than Triethylaluminum, or by an easier synthesis of Triethylaluminum.

There is a suggestion that there may be an industrial synthesis of triethylaluminum, that utilizes only Al+H2+Ethylene.

http://books.google.com/books?id=j3AwCqvqIzEC&pg=PA1122&...
View user's profile View All Posts By User
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 5-4-2009 at 03:01


Did you read my last few posts?

Starting from Al + EtX only, no alloy, you get quant. yield of an equal mixture of EtAlX2 and Et2AlX. In the case of X = Cl or Br, these are impractical to fractionate, but X= I can be fractionated. So one possibility is to use EtI.

EtCl and EtBr are cheaper, and in this case, adding NaCl to the mixture (say 1,1 mol per mol of EtAlX2) and heating produces a solid comples NaEtAlCl3 from which the Et2AlCl can be distilled.

Or reduce the mixture with Na and distill of the Et2AlCl

Whichever choice, you can now reduce the Et2AlX with Na and obtain Et3Al.

If you do not yet have sufficient Et3Al, you can just make more of the mixture from Al and EtX and now you can forget about NaCl, Na metal, and fractionation because Et3Al reacts with both components of the mixture to produce, for every mol reacted, 3 mols of Et2AlX.

Well, actually it is only reacting with EtAlX2 in a disproportionation but the net result is 2 new mols of Et2AlX and the mol that was already there, so 3 mols.

NOW reduce with Na and you get 2 mols Et3Al (and some NaCl).

My point is that the alloy is a luxury not a necessity.

The technical challenge is to be competent at airless procedures.

The exonomic hurdle is having the requisite autoclave - I do.

The easier prep of LiAlH4 is the one from LiH and AlCl3 in ether.

But we decided is was wasteful of LiH.

I do not think the hydroaluminolysis of ethylene is a bench scale procedure. In any case the process uses selfsame triethylaluminum as catakyst. Back to square one.

What we maybe can ask ourselves is whether Li wire, melted in paraffin oil and dispersed as sand, will take up H2 under pressure? If so then making LiH is easy and the wastefulness issue goes away.



[Edited on 5-4-2009 by Sauron]




Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 5-4-2009 at 07:36


The following is the abstract of the Ziegler article from Annalen 629 (1960) pp 33-49. Thanks fo Formatik for prompt amd excellent translation

Aluminium trialkyls form complex compounds of the coordinative 4-count aluminium of the sort M[AlR3X] (M= alkali metal, X = halogen, cyanogen) with many alkali halogenides as well as with alkali cyanides (and evidently generally -pseudohalogenides). Their stability increase with the ionic volume of the alkali metal, and decrease with increasing size of the halogen as well as the alkyl of the aluminium. The complex formation is restricted by lithium to (analgous to the halogenides) lithium hydride. For trimethyl and -triethylaluminium, it is without exceptions under the fluorides and cyanides of sodium to cesium. Under the chlorides, it is restricted to K, Rb, Cs and under the bromides, to Rb and Cs. Complexes of alkali iodides do not exist, though those of tetralkylammonium iodides do. - The stability relationships of the halogenide complexes can be taken out of plausible basic suppositions of relations of the lattice energy of the alkali halogenides and are pointed to without contradiction. - In addition to the 1:1 complexes, 1:2 complexes of the kind MX.2 AlR3 (X = H, F, Cl, CN) exist. Both aluminium trialkyls are bound variously strong in those. All of these compounds are electrolytes, however the 1:1 complexes of the alkali fluorides show only around 1/100 of the conductivity of the 1:2 complexes and the other alkali halogenide complexes. - The complex compounds, NaF.Al(CnH2n-1)3 and NaF.2Al(CnH2n+1)3, are proven up to n = 4, after n = 6 they are certainly unstable. Further on up in the homologous rows can be achieved with potassium fluoride. - Principally, similar laws apply to the alkali halogenide complexes of R2Al.halogen. M[AlR2Cl2] exists when M = K, but not when M = Na. - Complex formation occurs further with carbonates and carbonic acid salts. However, these complexes are unstable and quickly change through intramolecular reactions.

Aluminiumtrialkyle geben mit vielen Alkalihalogeniden sowie mit Alkalicyaniden (und offenbar allgemein -pseudohalogeniden) Komplexverbindungen des koordinativ 4-zähligen Aluminiums vom Typ M[AlR3X] (M = Alkalimetall, X = Halogen, Cyan). Ihre Stabilität nimmt mit dem Ionenvolumen des Alkalimetalls zu, mit dem des halogens sowie mit der Größe der Alkyle am Aluminium ab. Die Komplexbildung beschränkt sich beim Lithium auf das (den Halogeniden analoge) Lithiumhydrid. Gegenüber Aluminiumtrimethyl und -triäthyl tritt sie bei den Fluoriden und Cyaniden von Natrium bis Cäsium ohne Ausnahme ein. Bei den Chloriden ist sie auf die des K, Rb und Cs, bei den Bromiden auf die des Rb und Cs beschränkt. Komplexe der Alkalijodide gibt es nicht, wohl aber solche von Tetraalkylammoniumjodiden. - Die Stabilitätsverhältnisse der Halogenidkomplexe lassen sich aus bestimmten plausiblen Grundannahmen heraus zu den Gitterenergien der Alkalihalogenide in Beziehung setzen und in sich widerspruchsfrei deuten. - Außer den 1 : 1-Komplexen existieren 1 : 2-Komplexe der Art MX·2 AlR3 (X = H, F, Cl, CN). Die beiden Aluminiumtrialkyle sind in ihnen verschieden fest gebunden. Alle diese Verbindungen sind Elektrolyte, jedoch zeigen die 1 : 1-Komplexe der Alkalifluoride nur rund 1/100 der Leitfähigkeit der 1 : 2-Komplexe und der anderen Alkalihalogenid-Komplexe. - Die Komplexverbindungen NaF. Al(CnH2n - 1)3 und NaF·2Al(CnH2n+1)3 sind bis n = 4 nachgewiesen, ab n = 6 sind sie sicher instabil. Weiter herauf in der homologen Reihe kommt man mit Kaliumfluorid. - Grundsätzlich ähnliche Gesetzmäßigkeiten gelten für die Alkalihalogenid-Komplexe von R2Al·Halogen. M[AlR2Cl2] existiert, wenn M = K, nicht aber, wenn M = Na. - Komplexbildung tritt weiter ein mit Carbonaten und carbonsauren Salzen. Die Komplexe sind jedoch instabil und verändern sich rasch durch intramolekulare Reaktionen.

[Edited on 6-4-2009 by Sauron]




Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 6-4-2009 at 03:42


A careful reading of the all important 1940 paper by Aristid V.Grosse (J Org Chem 5, 106) provides the important reminder that the sodium reduction of ethylaluminum "sesquihalide" can proceed to the triethylaluminum in one step without isolation and puridication of the intermediate reduced diethylaluminum halide.

The reduction of the sesquigalide mixture to Et3Al proceeds with a yield of 40-50% while the Ba reduction of pure Et2AlX2 has a yield of 60%.

The "shortcut" reduction is according to the following equation

Et3Al2X3 + 3 Na -> Et3Al + Al + 3 NaX

Any excess of Na must be carefully avoided in order to preclude formation of the nonvolatile tetraethylaluminum compound.

So this simplification allows a shorter route from Al metal and alkyl halide.

If the Mg/Al alloy is on hand then its use affords Et2AlX2 directly and the overall yield from starting materials is slightly higher, but not enough to make acquisition or preparation of the alloy absolutely vital

Furthermore according to Grosse the disproportionation of sesquiha;ide with R3Al proceeds to a 77% yield. Since this affords Et2AlX which still must be reduced with Na to get Et3Al, it is clear that the product of these yields (77% x 60%) is little better than the 40-50% yield of the Na reduction of sesquihalide to trialkylaluminum.

The Grosse paper is posted by me on page 2 of the Parr Shaker Hydrogenator thread if anyone wants recourse to it.

[Edited on 6-4-2009 by Sauron]




Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
panziandi
Hazard to Others
***




Posts: 490
Registered: 3-10-2006
Location: UK
Member Is Offline

Mood: Bored

[*] posted on 6-4-2009 at 04:04


This link provides data regarding sodium aluminium hydride. It also shows relative reaction rates for reduction of groups with SAH vs LAH

http://www.albemarle.com/TDS/Fine_chemistry_services/SC2035F...




View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 6-4-2009 at 06:24


Thanks, that ought to be useful.

EtAlCl2 is a strong Lewis acid and a useful catalyst for ene reactions between aldehydes and alkenes. This is in contrast to the MeAlCl2 which is a weak Lewis acid. Go figure.

[Edited on 6-4-2009 by Sauron]

Attachment: jo00152a011.pdf (207kB)
This file has been downloaded 1288 times





Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 8-4-2009 at 20:30
Update


The acquisition of custom alloy turnings 69% Al 31% Mg ("magnalium") is moving ahead, I am in touch with a UK source and his prices are reasonable. We are ironing out some details.

This w/w% amounts to 2 g-atoms Al and 1 g-atom Mg as required by the stoichiometry for the prep and reduction of Rt3Al2X3 to Et2AlX (X = Cl, Br, I).


Magnalium.jpg - 19kB

[Edited on 9-4-2009 by Sauron]




Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
benzylchloride1
Hazard to Others
***




Posts: 299
Registered: 16-3-2007
Member Is Offline

Mood: Pushing the envelope of synthetic chemistry in one's basement

[*] posted on 10-4-2009 at 21:13


This is a fascinating way of making sodium and lithium aluminum hydrides. I would advise handling aluminum alkyls in a glove box or with a vacuum line because of their spontaneously flammable nature. I have some experience with working with air sensitive compounds. How do you plan to handle the triethylaluminum? Do you have a glove box and high vacuum line? I am currently aquiring the glassware and equipment to construct my own high vacuum line. I have a single bank manifold, but it is not the ideal setup. I am planning on buying a used glove box off of Ebay. There is a seller that has listed several times a glove box that is in good condition for around $400. I would buy it if I had the money. The glove box listed for $7000 new in a recent Cole Parmer catalog.



Amateur NMR spectroscopist
View user's profile View All Posts By User
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 10-4-2009 at 21:28


Yes I have a full size airlock equipped lighted and electrically serviced Labconco glove box equipped for Ar or N2.

I also have the requisite autoclave (Parr 1 liter SS316 stirred and heated with temp controller and T/C. This unit is rated 1900 psig @ 350 V, Overkill for this reaction.

The triethylaluminum will be stored in steel or SS sample cylinders with Swagelok diaphragm valves, filled in the glove box, and aliquots drawn by gastight syringe in the glove box.




Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
benzylchloride1
Hazard to Others
***




Posts: 299
Registered: 16-3-2007
Member Is Offline

Mood: Pushing the envelope of synthetic chemistry in one's basement

[*] posted on 10-4-2009 at 22:00


I am planning on buy one of the portable plexiglas type glove box as I cannot afford one of the more expensive types. How well do these type of glove boxes work for handling highly air sensitive materials. The one I was looking at on Ebay has an air lock and electrical services. Plexiglas does not hold up well with organic solvents so I will have to be extremly cautious when I obtain one of these glove boxes to avoid damage to it by spilled solvents.



Amateur NMR spectroscopist
View user's profile View All Posts By User
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 10-4-2009 at 23:54


In addition to the airlock this has a large door to allow karger equipment in and out, I would set one or more teflon or SS trays in the bottom to protest the fiberglass floor.

Plexiglass is acylic. DCM is solvent for acrylic and is how you glue acrylic together. So rule #1 with an acrylic box is: no DCM spills. Check the chemical compatibility tables for other solvents and reagents.

I paid $400 for my box, the shipping from Missouri to SF CA was truck and then it went ocean to Bangkok. I probably have $15900 in it nit counting new gaintlets $400 so these things are not cheap.

You know the drill, pump the box out then flush it with dry B2 or Ar depending on what you will work with, the gas needs to be dry and O2 free (use catalytic traps.) Repeat the purge and flush till an indicator inside shows no moisture and no O2.

The airlock has its own gas controls so it can be purged and flushed independently. That is the point.

Depending again on the task at hand, you either run the box at skughtky positive pressure to mantain the integrity of the inert dry atmosphere.

Or at a slight negative pressure when using the box as a containment for say carcinogen, or otherwise obnoxious materials. This way any leaks are inbound.

The most usual gauntlets are neoprene, and you wear cotton lab gloves under to absorb sweat.

[Edited on 11-4-2009 by Sauron]




Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
benzylchloride1
Hazard to Others
***




Posts: 299
Registered: 16-3-2007
Member Is Offline

Mood: Pushing the envelope of synthetic chemistry in one's basement

[*] posted on 13-4-2009 at 21:27


I located a Labconco carcinogen handling glove box on Ebay for $220. I am wondering if this box would work for inert atmosphere work. It has a blower attached to the top of it. The box seems to be in excellent condition with gloves and has an air lock with a larger door which would be helpful. The plexiglas one does not have the large door. I will continue to watch and will buy when the I find the best deal. Until then I will be putting together a vacuum line. The Parr reactors seem to be out of my price range currently.



Amateur NMR spectroscopist
View user's profile View All Posts By User
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 13-4-2009 at 21:51


It depends on what fittings the box comes with, I would not count on the gloves being in serviceable condition.



Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
aliced25
Hazard to Others
***




Posts: 262
Registered: 31-7-2010
Member Is Offline

Mood: No Mood

[*] posted on 19-5-2013 at 04:19


Aluminium hydride can be hydrogenated directly to Aluminium Hydride (AlH3).

LiH can be turned into LiAlH4 with a Ti.doped AlH3 solution in THF (Et2O doesn't work).

The pressures are 32 bar for the AlH3 production at 300K and RT, 13 bar for the catalyzed reaction.

Given I've shown elsewhere that it is possible to produce 99.9% H2 at up to 100 bar, surely someone can work out the rest? I can grab the diagrams of the Parr Reactors they are using - the magnetic stirrer mechanism isn't exactly rocket science.

Attachment: Graetz.etal.Regeneration.of.LiAlH4.pdf (919kB)
This file has been downloaded 630 times

Attachment: IV.H.12.Atomistic.Transport.Mechanisms.in.Aluminium.Based.Hydrides.pdf (465kB)
This file has been downloaded 627 times

Attachment: Graetz.Reilly.Wegrzyn.Direct.Hydrogenation.of.Aluminium.at.Low.Pressure.pdf (202kB)
This file has been downloaded 597 times

[Edited on 19-5-2013 by aliced25]




From a Knight of the Realm: "Animated movies are not just for kids, they're also for adults who do a lot of drugs." Sir Paul McCartney
View user's profile View All Posts By User
Bot0nist
International Hazard
*****




Posts: 1559
Registered: 15-2-2011
Location: Right behind you.
Member Is Offline

Mood: Streching my cotyledons.

[*] posted on 19-5-2013 at 05:51


This is all extremely intresting chemistry, and it would be quite a feat for an amatuer to pull off these industrial routes at home. Unfourtunatly, it is way beyond my scope, so I will just continue to buy it from Elemental. I know its expensive, and paying for that exemption packaging sucks, but when I need some LAH, thats the route I take...



U.T.F.S.E. and learn the joys of autodidacticism!


Don't judge each day only by the harvest you reap, but also by the seeds you sow.