BaCO3 from BaSO4 + C (1000 [Celsuis])
I want to try the BaCO3 - making from BaSO4 and charcoal. My furnace gives 1050 [Celsius]. Is that enough?
I would powder the charcoal, mix it 2:1 (stoechiometric) with the BaSO4-powder and heat it a while; but there are reports of BaSO4 as an oxidizer for
metal-powders: Is it safe with C ?
The BaS then I might as well directly react with some acid, instead of making BaCO3 first ? How to capture and dispose off the H2S? Soda ?
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Carbon reductions are much calmer than with reactive metals. Be more concerned about the fluidized bed sort of reaction you'll get. Something fluffy
plugging the crucible (*cough* kaowool) would help in that regard.
H2S can be absorbed effectively in NaOH/KOH solution. I would imagine suckback prevention and all that is a good idea. Then whatever gasses remain,
run through a flame so it's at least somewhat less poisonous SO2.
Tim
|
|
chloric1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1089
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline
Mood: Stoichiometrically Balanced
|
|
I think I read the classic book Inorganic preparations that the temperature necessary was closer to 1300 C. If it helps this is yellow heat
transitioning to white heat. A well engineered gas flame would be better. I would recommend you take your sulfate with charcoal and add some organic
binder and make "biscuits" that can be dried with low heat. Then use a really hot gas flame or oxyacetylene torch and heat the biscuits until they
disintigrate into a gray powder this will be your sulfide. In industry, yields are 70% so don't expect complete conversion.