Adsorption capacity of activated carbon?
I just recently became interested in solar powered adsorption refrigeration, (I'm that kind of guy). Of the adsorption systems out there ( CaCl2
/ammonia, carbon/ammonia, carbon/methanol, zeolite/water ...) the most accessible for the home experimenter would seem to be activated carbon/
methanol, as both are easy to get and easy to handle.
What I'm trying to work out is the methanol adsorption capacity of the carbon. The datasheets for the carbon usually specify an Iodine number for
adsorption capacity - can anyone tell me how that would relate to methanol adsorption? I'm only after a rough estimate so I will know if a kg of C
will handle a kg , or 100g , or 1g of MeOH.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
solo
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3973
Registered: 9-12-2002
Location: Estados Unidos de La Republica Mexicana
Member Is Offline
Mood: ....getting old and drowning in a sea of knowledge
|
|
Reference Information
Study of the performance of activated carbon–methanol adsorption systems concerning heat and mass transfer
L. W. Wang, J. Y. Wu, R. Z. Wang, Y. X. Xu, S. G. Wang and X. R. Li
Applied Thermal Engineering,Volume 23, Issue 13, September 2003, Pages 1605-1617
Abstract
Three types of adsorbers and two types of activated carbon–methanol adsorption systems are studied, and the structure of adsorbers, performance of
adsorbents, performance of different adsorbers and different systems are compared. Results show that the heat transfer coefficient of solidified bed
are much higher than that of granular bed, the design of gas flow channels in adsorbers is very important to the performance of mass transfer and the
performance of the whole system. Performance of the adsorber with good design of gas flow channels is much better than that of other two types of
adsorbers.
Attachment: Study of the performance of activated carbon–methanol adsorption systems concerning heat and mass transfer.pdf (415kB) This file has been downloaded 5250 times
It's better to die on your feet, than live on your knees....Emiliano Zapata.
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1314
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
Thanks Solo. Looks like the ballpark figure is around 0.22kg/kg.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
Tacho
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 582
Registered: 5-12-2003
Member Is Offline
Mood: No Mood
|
|
I have been very interested in this same topic over the last two weeks. I even built a device to make some basic tests. It consist of two metal tubes
connected by a PVC tube on the top. One is filled with activated carbon as a fine powder and the other with 50ml of methanol. I heated the carbon tube
for about half an hour at 110ºC and connected it to the PVC "bridge". Nothing happened. There has to be some extra trick. I think it may be the use
of some vaccum or of granulated cabon.
I'll read solo's paper to see if I find any new info.
Some papers on the subject:
http://www.sjtuirc.sjtu.edu.cn/news/ISHPC%20-%20101%20K.pdf (very good)
http://www.sjtuirc.sjtu.edu.cn/news/060912%EF%BC%882%EF%BC%8... (is that a link or what!)
http://www.cibse.org/pdfs/development.pdf
https://txspace.tamu.edu/bitstream/1969.1/5445/1/ESL-IC-06-1...
http://igt.heig-vd.ch/web/IMG/pdf/article_pour_site_internet...
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
Either pumping it down or heating the methanol so as to fill most of the space with MeOH vapour before sealing it up will help. Otherwise you are
going to have to wait for vapour to diffuse the length of the air-filled tube before it can be absorbed.
You'll want a lot of surface area for the methanol, and similarly you don't want to have the vapour to fight its way through saturated carbon to reach
carbon that can absorb it. And it's not quick, if you don't insulate the methanol evaporator you may not see much of a cooling effect on the small
scale of your test.
Something similar has been made to work using metallic 'sponge' instead of activated carbon, working as a "heat diode" that takes advantage of the low
temperature of the night sky to condense the working fluid, which runs back into the evaporator.When the sun is up, the vapours don't condense and
there is no flow from the evaporator/cold side to the radiator.
|
|
roamingnome
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 363
Registered: 9-9-2006
Member Is Offline
Mood: No Mood
|
|
you may have seen this article, but this guy is on it.....
http://www.solarhaven.org/AmmoniaAbsorptionIcemaker.pdf
|
|
Tacho
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 582
Registered: 5-12-2003
Member Is Offline
Mood: No Mood
|
|
By the way,
my activated carbon is too fine. So fine that it forms a black cloud that lingers in the air every time I use it. This is very annoying.
I would appreciate any suggestion of a binder that does not interfere with its adsorbing properties.
I was thinking of a small ammount of gypsum or maybe sodium silicate.
[Edited on 29-8-2007 by Tacho]
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1314
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
Everything I've seen so far concentrates on getting good heat transfer through the carbon, and short vapor pathways. I think you are going to need
granulated or pelletised carbon.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|