FA polymerization
A paper says Furfuryl alcohol can be polymerized, but no details.
I wonder what is the suitable polymerization condition for furfuryl alcohol, at what temperature?
someone says the acid is advantageous for polymerization, liquid acid is OK, but for solid acid such as zeolite is it OK?
any suggestions are welcome!
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Wikipedia says it's acid catalysed.
One might suppose, given the double bonds, that it could react via radical substitution (as other polyolefins are), but I'm supposing there are good
reasons why this doesn't work, or is grossly impractical.
Tim
|
|
vulture
Forum Gatekeeper
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
You can bet your ass that acid catalyzed polymerizations are never of radical nature. You're probably looking at a cationic mechanism.
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
guy
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 982
Registered: 14-4-2004
Location: California, USA
Member Is Offline
Mood: Catalytic!
|
|
As you can see, furfural has a nice aldehyde, which when protonated is a good electrophile. Then the other furfurals have pi bonds which can act as
nucleophiles. According to an article on furfural I have, the 5-carbon will be the nucleophile
|
|
Fleaker
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
Shucks, this polymerization might be why it's used in in phenolic resin casting sands. As I recall, the binder is phosphoric acid.
One can order furfuryl alcohol by the gallon for pretty cheap from a foundry supply house...
Neither flask nor beaker.