A Co3O4 FE cathode for Sauron's Accelerator


Now that Rosco has expounded so much on Cobalt and got me looking into it, I came across this article (attached)describing the synthesis and testing of Co3O4 "nanowalls" as field emitters.

The vertically oriented Co3O4 nanowalls were prepared "by a surprisingly simple method: directly heating Co foil on a hotplate under ambient conditions".

I don't know how rugged the stuff would be under ion bombardment, but it's interesting to think about it.

Attachment: Cobalt_Oxide_Field_Emitter.pdf (374kB)
This file has been downloaded 692 times