Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Finding amount of cobalt in Li ion batteries
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 12-8-2018 at 09:26
Finding amount of cobalt in Li ion batteries


LIBs capacities usually have a unit of mAh (0.001Ah).
1Ah=3600C.
For every C there's 6.24150934(14)×10^18 electrons.
Hence 1Ah=2.2469433624×10^22 e-
That's 0.0373mol
If 2LiCoO2 ↔ 2Li0.5CoO2 + Li+ + e-
Then for every mol of e- there's 2 mol Co atoms
That's 0.0746mol Co
Molar mass of Co=58.933gmol-1
Hence 1Ah=4.398g of Co
If LiCoO2 ↔ CoO2 + Li+ + e-
Then for every mol of e- there's 1 mol Co atoms
Hence 2.199g of Co
Therefore mass of Co is between 2.199 and 4.398g per Ah.

Is my calculation correct?

[Edited on 12/08/18 by fusso]




View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8013
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 12-8-2018 at 11:44


Yes, your computation looks fine. Of course, under the assumption that all "charge" is in the form of LiCoO2. In fact, in your scheme, it is cobalt giving charge, going from oxidation state +3 to oxidation state +4.

EDIT: On second thought, I have some doubts with this. Cobalt normally has oxidation state +2 and in some complexes it has oxidation state +3. But is there also a form of oxidation state +4? Apparently there is in the form of CoO2. Learned something new again ;)




[Edited on 12-8-18 by woelen]




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
AJKOER
Radically Dubious
*****




Posts: 3026
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 6-9-2018 at 06:14


See, possibly relatedly, the example of associated reactions occurring in a copper metal-air-ammonia electrochemical cell at https://onlinelibrary.wiley.com/doi/pdf/10.1002/bbpc.1963067... .

Interestingly, in the Cu/O2/NH3 cell there are two electron sources. One arises from the creation of a complex with ammonia with copper moving from +2 to +1 in oxidation states. However, the recycling equilibrium reaction:

Cu(2+)L + Cu = 2 Cu(+)L' (L= a NH3 ligand)

is needed to keep generating the added electron per the reaction:

[Cu(NH3)2] (+) + 2 NH3 --> [Cu(NH3)4] (2+) + e-

In my opinion, yes there could be some added electrons also formed in the Li/Co cell, but not likely as significant unless there is also some recycling equilibrium (perhaps even elemental cobalt presence as wishful thinking...).

As a side note, in the case of the Cu/O2/NH3 reaction system, those added electrons are, per my suspicion, the reason for the creation of nitrite (as in the NH4NO2 side product) in the active presence of oxygen, so perhaps not without potential chemical consequences.

[Edited on 6-9-2018 by AJKOER]
View user's profile View All Posts By User