Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Cleaning sintered glass filter from super tiny graphite mess.
TheMrbunGee
Hazard to Others
***




Posts: 364
Registered: 13-7-2016
Location: EU
Member Is Offline

Mood: Phosphorising

[*] posted on 15-6-2018 at 08:59
Cleaning sintered glass filter from super tiny graphite mess.


I ruined my filter with graphite particles, I was hoping to remove that stuff with hot piranha-ish solution (-ish - because I have only 10% H2O2)

It is now sitting there for a while, cooled, of course but it haven't got even a bit whiter.

Is there any other way?


Filter works fine, it is just esthetics.. And the challenge, maybe..




View user's profile Visit user's homepage View All Posts By User
SWIM
National Hazard
****




Posts: 970
Registered: 3-9-2017
Member Is Offline


[*] posted on 15-6-2018 at 09:13


I've heard dichromate and sulfuric acid can clean that, but I've never tried it.



View user's profile View All Posts By User
TheMrbunGee
Hazard to Others
***




Posts: 364
Registered: 13-7-2016
Location: EU
Member Is Offline

Mood: Phosphorising

[*] posted on 15-6-2018 at 09:41


Ok, that's a possibility! I don't have any dichromates on me, so I will wait for confirmation, before I drive after some.



View user's profile Visit user's homepage View All Posts By User
Texium
Administrator
********




Posts: 4581
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: PhD candidate!

[*] posted on 15-6-2018 at 09:46


Quote: Originally posted by SWIM  
I've heard dichromate and sulfuric acid can clean that, but I've never tried it.
I've done it. It works quite well, though I prefer using piranha now that I have 27% peroxide since it's much safer and easier to dispose of.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
TheMrbunGee
Hazard to Others
***




Posts: 364
Registered: 13-7-2016
Location: EU
Member Is Offline

Mood: Phosphorising

[*] posted on 15-6-2018 at 09:54


Okay, thank You both! :)



View user's profile Visit user's homepage View All Posts By User
unionised
International Hazard
*****




Posts: 5126
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 15-6-2018 at 15:05


You can remove graphite using air.

You may need to heat the item to get a reaction rate you are happy with.
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 16-6-2018 at 00:56


Quote: Originally posted by Texium (zts16)  
Quote: Originally posted by SWIM  
I've heard dichromate and sulfuric acid can clean that, but I've never tried it.
I've done it. It works quite well, though I prefer using piranha now that I have 27% peroxide since it's much safer and easier to dispose of.


Easier to dispose of, yes certainly. But it’s not safer. Far from it. There have been numerous serious lab accidents resulting from the use of piranha solution.

I’ve had luck removing activated carbon powder from frits using piranha made with drain cleaner acid and 12% hydrogen peroxide. I assume graphite powder is more difficult to remove due to surface area to mass ratio, but it should still work slowly I think.

One good think about chromic acid is that you can reuse it indefinitely - piranha goes off pretty quickly and must be prepared immediately before use.




View user's profile View All Posts By User