aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 19-3-2018 at 12:43


Unfortunately nobody can claim to be the Best Chemist Ever, nor can quick experiments show the Full story.

Sn has a horrible tendency to form metastannic acid under those conditions, given Time.

It's like snot.

http://goldrefiningwiki.com/mediawiki/index.php/Metastannic_...




View user's profile View All Posts By User
XeonTheMGPony
International Hazard
*****




Posts: 1640
Registered: 5-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 19-3-2018 at 15:54


Quote: Originally posted by CobaltChloride  
Quote: Originally posted by XeonTheMGPony  
Quote: Originally posted by CobaltChloride  
I also want to separate these metals. Is it a viable option to dissolve it in nitric acid which would create solution of lead nitrate and SnO2? How would I go about reducing SnO2 to Sn metal (besides reduction with charcoal)?


electrochemicaly be easiest method,

How would I do that with this insoluble compound?


look at codies lab video it works very well the lead gunk then can be melted and used for what ever or tin for what ever, Tin will be useless for me but I'll make lead acetate via 35%H2O2 and glacial acetic acid
View user's profile View All Posts By User
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 20-3-2018 at 00:25


@Akhil:

SnCl4 could probably present in soln so it didnt ppt out.
View user's profile View All Posts By User
CobaltChloride
Hazard to Others
***




Posts: 239
Registered: 3-3-2018
Location: Romania
Member Is Offline


[*] posted on 20-3-2018 at 02:28


Quote: Originally posted by aga  
Unfortunately nobody can claim to be the Best Chemist Ever, nor can quick experiments show the Full story.

Sn has a horrible tendency to form metastannic acid under those conditions, given Time.

It's like snot.

http://goldrefiningwiki.com/mediawiki/index.php/Metastannic_...

Well that's good for this separation because it means we have lead in solution and tin as a precipitate. But the question about reducing it to Sn metal still remains (besides using charcoal as that has a tendency to dissolve in molten metal, thus making impure tin).

[Edited on 20-3-2018 by CobaltChloride]
View user's profile View All Posts By User
yobbo II
National Hazard
****




Posts: 747
Registered: 28-3-2016
Member Is Offline

Mood: No Mood

[*] posted on 20-3-2018 at 08:14


https://www.sciencemadness.org/whisper/viewthread.php?tid=54...