Separatory Funnel O-Rings


I recently lost an O-Ring for my separatory funnel’s stopcock down the drain. I am looking to buy a replacement, but I am unsure what type of O-Ring will provide the chemical resistance that is necessary. It needs to be able to withstand many organic solvents as well as acidic and basic solutions. Will Buna-N or Viton be sufficient? Or does it need to be something more substantial like PTFE or Chemraz?



Check out my YouTube channel! www.youtube.com/user/gooferking
View user's profile Visit user's homepage View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 11-1-2018 at 09:01


I would try the O-rings from Ace Hardware. I think they are made of Viton.



The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 11-1-2018 at 16:36


I also think Viton would work well. It is almost as resistant to chemicals and temperature extremes as PTFE.



View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4583
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: PhD candidate!

[*] posted on 11-1-2018 at 16:48


At work, I have nitrile (NBR), HNBR, and Viton O-rings. They all work fine, but the HNBR and Viton seem to be more durable for long term use than the nitrile ones, which begin to wear out over time.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
XeonTheMGPony
International Hazard
*****




Posts: 1640
Registered: 5-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 11-1-2018 at 17:28


Viton is used in most HVAC gear, where it is exposed to some pretty nasty conditions.
View user's profile View All Posts By User
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 12-1-2018 at 19:35


I been using these with vac high temp grease. They are on ebay and ALL 4 boxs were sold together for £4
https://www.ebay.co.uk/itm/419pc-Rubber-O-Rings-Tap-Washers-...
20180113_032951[1].png - 1.1MB 20180113_033026_-_Copy[1].png - 1.2MB

[Edited on 13-1-2018 by NEMO-Chemistry]
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2736
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: No Mood

[*] posted on 12-1-2018 at 20:06


Great find Nemo, I paid a lot for a box of them years ago. But I always run out of the smaller ones for stopcocks whenever I have an assortment. Viton is fine for most chemicals, the O-ring should not see much solvent if the stopcock does not leak.
View user's profile View All Posts By User
PiledhigherandDeeper
Harmless
*




Posts: 17
Registered: 17-3-2013
Location: USA
Member Is Offline

Mood: No Mood

[*] posted on 13-1-2018 at 06:36


Quote: Originally posted by Dr.Bob  
Great find Nemo, I paid a lot for a box of them years ago. But I always run out of the smaller ones for stopcocks whenever I have an assortment. Viton is fine for most chemicals, the O-ring should not see much solvent if the stopcock does not leak.


Dr. Bob (and ALCON)

https://www.harborfreight.com/180-piece-viton-o-ring-kit-675...

Picked these up for 10 bucks at HF yesterday. Granted you get 5-10 of numerous sizes, the price is right for me. A 50 pack of one size is about the same price at McMaster Carr; I suppose it depends on how many of one size you go through.

Magpie,

Thanks for the tip about Ace. I am really developing a strong love for Ace Hardware and how they provide under the radar items for hobbyists.
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 13-1-2018 at 06:48


You're welcome. One member said that Ace is a chemical supplier masquerading as a hardware store.



The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 13-1-2018 at 08:13


Quote: Originally posted by Magpie  
You're welcome. One member said that Ace is a chemical supplier masquerading as a hardware store.

We have a crap hardware store! But seriously from a UK perspective, i can honestly say the above quote could be nearer the truth than you think.

Regulations would be less, plus its easy to justify alot of chems for a hardware/DIY type use. But set a Chemical company up and try and sell hardware would not be so easy.

Your equiv to our SIC numbers would make it hard for a chem company to sell Hardware, but the SIC numbers are not difficult to switch around so a hardware company could sell alot of chems.
View user's profile View All Posts By User
PirateDocBrown
National Hazard
****




Posts: 570
Registered: 27-11-2016
Location: Minnesota
Member Is Offline

Mood: No Mood

[*] posted on 13-1-2018 at 11:01


A while ago, California had a restriction on sale of MEK, I'm assuming for air quality reasons. So, WM Barr, the main maker of it for consumer purposes, came out with "MEK substitute" for a short time. It was ethyl acetate, in inexpensive gallon quantities. Later, the restriction was reversed, and Barr went back to MEK and discontinued the substitute.

But my local ACE has both on the shelves! Gotta love it.