Chromium Sulphate from Stainless Steel


I'm trying to make Chrome Alum from stainless steel as a starting material, but I am having trouble separating chromium sulfate from the ferrous sulfate.

The resulting mixture from reacting stainless steel with dilute sulfuric acid is two parts: one is a dark liquid and the other a green slushy-like material. The dark liquid portion clearly has some ferrous sulfate in it.

Is there any way to separate the two compounds while leaving the chromium sulfate in tact?
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4334
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 28-6-2017 at 15:49


Isolation of chromium compounds from stainless steel has been discussed in other threads.

I suggest sodium hydroxide. Cr forms a soluble complex ion; Fe does not.




Please remember: "Filtrate" is not a verb.