If someone wanted to mill a bunch of different samples of something like BP say 10-20g, would a small container of about 2-2.5" diameter by 2.5" tall work for milling? It would fill the container about 1/4 full, maybe 1/5. I just don't know if there is a minimum diameter that works for milling. I figure something larger might not allow for enough contact but am concerned as to whether there is some practical limitation to size due to some physics related to ball milling. As far as rotational speed, that can be adjusted to whatever is ideal for the process.
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 20-2-2017 at 02:38


Like anything related to dynamic and flow of liquids or dusts ... scaling up or down is not easy matter.

There is somewhere on this forum a document that was posted by another user about the dimensional study and rotational speed of ball millers...but I can't find it back...maybe someone else will be able to do that.

I think that the best is to try...doesn't cost much and you will get an answer faster.

But I really think that below a certain level ball milling becomes less efficient than hand:
-pestel and mortar
-grinding between two hard planes (like spatula and granit surface..as it is done into pharmacy)




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
RogueRose
International Hazard
*****




Posts: 1590
Registered: 16-6-2014
Member Is Offline


[*] posted on 20-2-2017 at 06:40


Quote: Originally posted by PHILOU Zrealone  
Like anything related to dynamic and flow of liquids or dusts ... scaling up or down is not easy matter.

There is somewhere on this forum a document that was posted by another user about the dimensional study and rotational speed of ball millers...but I can't find it back...maybe someone else will be able to do that.

I think that the best is to try...doesn't cost much and you will get an answer faster.

But I really think that below a certain level ball milling becomes less efficient than hand:
-pestel and mortar
-grinding between two hard planes (like spatula and granit surface..as it is done into pharmacy)


Can the particles get as small in a mortar & pestel as with a ball mill?

The reason I was thinking about the small container was b/c I could place 6-8 on the mill at a time, for different mixtures or recipes.
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1698
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 20-2-2017 at 08:22


Lloyd Sponenburgh published a booklet some years ago that covered everything you need to know about ball mills for BP. I'm sure you can find it if you do a search for it.





We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 20-2-2017 at 14:13


Quote: Originally posted by RogueRose  


Can the particles get as small in a mortar & pestel as with a ball mill?

The reason I was thinking about the small container was b/c I could place 6-8 on the mill at a time, for different mixtures or recipes.

Yes by hand and with the proper tools you can go as small/fine as with a ball mill.

I understand the idea...nice...so you can get exactly the same ball milling time and conditions in parallel.




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
wg48
National Hazard
****




Posts: 821
Registered: 21-11-2015
Member Is Offline

Mood: No Mood

[*] posted on 20-2-2017 at 17:45


In a tumbler type ball mill your small diameter would mean the balls are not falling very far and its rotating slowly compared to a larger diameter. I guess you could off set that effect by using dense media. It may take a long time to mill your material.


Perhaps you need a planetary or vibratory ball mill. A vibratory mill should be easy to build compared to a planetary one. The noise could be high though but apparently they are very quick. If the vibration is linear so the jar does not rotate perhaps it could be used to make hydrides easily.
View user's profile View All Posts By User