[*] posted on 26-1-2017 at 09:44
Make aluminium powder of 60~30 µm


I need make aluminium powder, however, produce it using common sandpaper in aluminium foil, although effective, is slow and impractical.
Also, produced aluminium powder has a pinky-gray colour due to impurities (pink for the colorant of sandspaper), ie, aluminium can tear to common sandpaper.
Also, I don't have coffee grinder nor other machine for create it.

What type of sandpaper can I use?

Is there better alternatives that doesn't implies the use of machines?

[Edited on 26-1-2017 by Steamboy]
View user's profile View All Posts By User
Jstuyfzand
Hazard to Others
***




Posts: 166
Registered: 16-1-2016
Location: Netherlands
Member Is Offline

Mood: Learning, Sorta.

[*] posted on 26-1-2017 at 12:57


A ball mill, closer to machineless is not going to happen.
If there is an alternative, I'd love to hear about it.
View user's profile View All Posts By User
Chlorine
Hazard to Self
**




Posts: 56
Registered: 26-11-2016
Location: Maine, USA
Member Is Offline

Mood: Brominated

[*] posted on 27-1-2017 at 02:50


Your best option is to buy or make a ball mill. Machined aluminum turnings work wonders because they're dirt cheap and brittle. I've tried using foil in a ball mill and it was a disaster.
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1685
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 27-1-2017 at 06:03


Maybe by heating a roll of aluminum foil and then quenching it, it would become less ductile or embrittled enough to use.
View user's profile View All Posts By User
gatosgr
Hazard to Others
***




Posts: 237
Registered: 7-4-2015
Member Is Offline

Mood: No Mood

[*] posted on 27-1-2017 at 12:53


You can also evaporate aluminum in vacuum and then quench it.



View user's profile View All Posts By User
Meltonium
Hazard to Self
**




Posts: 97
Registered: 23-9-2016
Location: Home in pajamas
Member Is Offline

Mood: Fluorinated

[*] posted on 27-1-2017 at 13:23


A nice, coarse file might work well instead of sandpaper. Although, it may be prone to clogging since aluminium is very soft.



"If at first you don't succeed, fail, fail again."