Oxalic Acid from Skunk Cabbage
The "greenbelt" behind my house is plagued by lots of Western Skunk Cabbage, which is known for having calcium oxalate crystals in it which makes it
poisonous. I was thinking that it might be possible to extract oxalic acid (which could then be purified by turning it back into calcium oxalate) by
steeping the leaves in a dilute solution of hydrochloric acid to turn the calcium oxalate into oxalic acid, adding calcium chloride to the filtered
solution to precipitate out calcium oxalate while leaving most of the other contaminants in solution, and then either using the calcium oxalate or
turning it back into oxalic acid with hydrochloric acid. If needed the oxalic acid could be separated from the calcium chloride in solution by
dissolving everything in ethanol (since oxalic acid is much more soluble in ethanol than calcium chloride), or acetone, although I haven't found
whether or not oxalic acid is soluble in acetone. Yes, I know I could just go buy oxalic acid, but I like finding impractical routes to chemicals just
because I can!
[Edited on 4-16-2015 by DFliyerz]
|
|
Bert
|
Thread Moved 16-4-2015 at 10:41 |
Bert
Super Administrator
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
You might have a cheaper/easier result from sawdust and mixed alkalis.
http://thesis.library.caltech.edu/487/
But hey, if it looks more interesting to do a plant extraction, by all means! Please do report your results.
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
DFliyerz
Hazard to Others
Posts: 241
Registered: 22-12-2014
Member Is Offline
Mood: No Mood
|
|
I'd probably do that method instead, but I don't have any potassium hydroxide! (I'm doing a small batch from potassium carbonate/calcium hydroxide,
but again; it's very small.)
|
|
j_sum1
Administrator
Posts: 6297
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Could the same be attempted with rhubarb leaves?
|
|
macckone
Dispenser of practical lab wisdom
Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
There are good extractions for rhubarb, just do a Google search. Hydrochloric acid may improve the mobility of calcium oxalate but it will not
improve the oxalate solubility. The calcium oxalate is still not very soluble.
|
|
j_sum1
Administrator
Posts: 6297
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Next time I grow (or see) rhubarb, I might give this a go.
|
|
Amos
International Hazard
Posts: 1406
Registered: 25-3-2014
Location: Yes
Member Is Offline
Mood: No
|
|
Your procedure sounds like it would work, but I would recommend adding calcium carbonate instead of calcium chloride to re-precipitate calcium
oxalate; this will ensure neither hydrochloric acid nor oxalic acid remain in solution.
Scrolling down far enough on this page, you'll find that oxalic acid is insoluble in acetone, but it is very soluble in ethanol.
For a few other DIY routes to oxalic acid, check out this page: http://www.henriettes-herb.com/eclectic/kings/acidum-oxal.ht...
|
|