[*] posted on 20-1-2015 at 17:40
Using Chemistry to Refine Gold - Gold Filled Scrap


Here is my latest video on the process I use to RECOVER gold from gold filled watch cases and gold filled jewelry, then I REFINE the recovered gold to a high purity.

https://www.youtube.com/edit?o=U&video_id=iMfolFC0Rr8

Critical comments for improvement would be appreciated!

kadriver
View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 20-1-2015 at 20:47



Quote:
(edit)

http://youtu.be/iMfolFC0Rr8 is a good link-


I get "no videos are currently available"

Having some familiarity with the classical processes as documented by Georgius Agricola in "De Re Metallica" (and later authors), I look forward to viewing your procedures...


[Edited on 21-1-2015 by Bert]




Rapopart’s Rules for critical commentary:

1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.

Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).

View user's profile View All Posts By User
violet sin
International Hazard
*****




Posts: 1477
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline

Mood: Good

[*] posted on 20-1-2015 at 21:02


that was very well done, I'm glad you went to all that trouble to make it, as I found that quite interesting

[Edited on 21-1-2015 by violet sin]
View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 20-1-2015 at 21:33


Let's try this?

http://youtu.be/iMfolFC0Rr8

Yes, well done. Appreciate the added emphasis on safety, specific mention of using fume hood & not improperly disposing of your liquid byproducts.


[Edited on 21-1-2015 by Bert]




Rapopart’s Rules for critical commentary:

1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.

Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).

View user's profile View All Posts By User
silverforgestudio
Harmless
*




Posts: 4
Registered: 25-3-2015
Member Is Offline

Mood: Tinkering with conventions and the rules of money

[*] posted on 22-4-2015 at 13:36


kadriver- what did you do with the watch movements? Broken or not- let me know- I wouldn't mind getting them for tinkering on!
View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 22-4-2015 at 14:02


Excellent video.

1. I'd hate to be Gold if that's what happens

2. Aren't the exquisite watches worth more ?




View user's profile View All Posts By User
Texium
Administrator
Thread Moved
22-11-2023 at 19:20

  Go To Top