How would I go about depolymerizing styrofoam to it's monomer? Would I need to add some kind of inhibitor? A colleague of mine once told me that it woud have to be done under nitrogen, but i'm no longer in touch with him, and i've no idea how I might go about it.
View user's profile View All Posts By User
runlabrun
Hazard to Others
***




Posts: 172
Registered: 4-12-2004
Member Is Offline

Mood: No Mood

[*] posted on 2-3-2006 at 20:05


im not sure how to do it, there was a big discussion of this a while back on another board which shall remain nameless. Best bet would be to buy those fibreglass kits and extract the un-polymerised styrene from the tub in the kit... its just styrene in a solvent and inidcator dye (to see when the sytrene is polymerising) but this too would have to be done under nitrogen and with very clean glassware, even then it would need to be stabilised in solution to prevent it polymerising post extraction.

-rlr
View user's profile View All Posts By User
solo
International Hazard
*****




Posts: 3971
Registered: 9-12-2002
Location: Estados Unidos de La Republica Mexicana
Member Is Offline

Mood: ....getting old and drowning in a sea of knowledge

[*] posted on 2-3-2006 at 20:06


Someone had the same idea back at the old Hive board.......and here is a reply from an elder bee...........solo


------------------------------------------------------------------------------------
Osmium
Member   posted 05-06-98 04:36 AM          
--------------------------------------------------------------------------------
Thermal depolymerization of styrene doesn't work, because you will get only a small percentage of styrene and lots of other shit.
But styrene is no problem to get, ask chem supplier (expensive), or buy from plastic resin supplier in gallon quantities (used in polyester resins).
 




It's better to die on your feet, than live on your knees....Emiliano Zapata.
View user's profile View All Posts By User
Flip
Hazard to Others
***




Posts: 116
Registered: 7-12-2005
Member Is Offline

Mood: No Mood

[*] posted on 2-3-2006 at 20:31
Depolymerization of Styrofoam


Oh, I wouldn't hesitate for a moment to place an order for a gallon of styrene monomer. I'm just rather fond of the idea of synthesizing my compound of interest starting with ordinary styrofoam. Bragging rights, you know. However, I would love to get a viable OTC source.

Speaking of the old Hive board, how can I get my hands on the archive? I mean, the whole forum archive, not the Rhodium archive. Does anyone have it who would send it to me?

Flip
View user's profile View All Posts By User
Polverone
Now celebrating 21 years of madness
*********




Posts: 3186
Registered: 19-5-2002
Location: The Sunny Pacific Northwest
Member Is Offline

Mood: Waiting for spring

[*] posted on 3-3-2006 at 00:10


I've done it on a test tube scale without difficulty. I first added packing peanuts to acetone to "melt" them, then let the compacted material dry. A small chunk of this material was heated over an open flame in a pyrex test tube. It melted/boiled easily and refluxed within the tube. I was able to pour the clear, slightly yellowish liquid off to another test tube if I let it cool for a few seconds. It smelled like styrene and was easily enough oxidized by permanganate like a sample of commercial styrene monomer.



PGP Key and corresponding e-mail address
View user's profile Visit user's homepage View All Posts By User
bio2
Hazard to Others
***




Posts: 447
Registered: 15-1-2005
Member Is Offline

Mood: No Mood

[*] posted on 3-3-2006 at 03:59


Patent written in Chinese.
Application: CN 94-119654 19941215. CAN 124:316760 AN 1996:285029
CAPLUS

Patent Family Information

Patent No. Kind Date Application No. Date
CN 1110677 A 19951025 CN 1994-119654 19941215

Priority Application
CN 1994-119654 19941215


Abstract

PhCH2CO2H (I) is prepd. from polystyrene (II). Crushed II was distd. at >
340° to give styrene, which was heated with S and NH4OH in EtOH at 93-95°
to give 94% PhCONH2. Hydrolysis of PhCONH2 with HCl in H2O gave 84% I.
This process is efficient and pollution-free.