I am trying to figure out what the reduction potential of silicon is, specifically Si+4 seeing as it is the oxidation state of silicon in SiO2. I can't seem to find it anywhere - in any book I look in there is a dash through the line in the table where it should be. Why hasn't anyone determined its reduction potential? It is such an abundant element. This is baffling me - any input would be great.
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 26-1-2006 at 16:06


Si(4+) doesn't exist in solution, AFAIK. SiF6(2-) might work though. I doubt SiO4(4-) or SiO3(2-) would work. Come to think of it, all of these species are pretty well equivalent, using a strongly electropositive component, no? And such ions tend not to reduce in H2O solution, don't they?

Best way to electrically reduce it would be like aluminum: from a salt melt. :(

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger

  Go To Top