Copper


Hi, i need copper in dust and i think that 2HCl + Cu -----> CuCl2 + H2 and then CuCl2 + Al ------> Cu + AlCl2 and then remove the AlCl2... is it possible???

thanks

Sorry by the new topic but i havenĀ“t found anything...

[Edited on 16-1-2005 by sathor]
View user's profile View All Posts By User
neutrino
International Hazard
*****




Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline

Mood: oscillating

[*] posted on 16-1-2005 at 12:55


It would be AlCl<sub>3</sub>, not AlCl<sub>2</sub>. This could work, as aluminum chloride is soluble. There is another thread on this where CuSO<sub>4</sub> and Vitamin C is used.
View user's profile View All Posts By User
cyclonite4
Hazard to Others
***




Posts: 480
Registered: 16-11-2004
Location: is unknown
Member Is Offline

Mood: Amphoteric

[*] posted on 17-1-2005 at 03:45


HCl doesnt react directly with Copper, the Cu has to be oxidised first, so you could react the oxide with acid, add an oxidising agent, or bubble air through the acid to aid dissolving the Copper.



\"It is dangerous to be right, when your government is wrong.\" - Voltaire
View user's profile View All Posts By User This user has MSN Messenger
chemoleo
Biochemicus Energeticus
*****




Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline

Mood: crystalline

[*] posted on 17-1-2005 at 05:48


THere's a multitude of threads on copper dissolution and so on. If'd like to discuss this please do so in the proper threads. Same goes for the copper powder - just follow neutrino's link.

Btw - Zn, and Fe powder was mentioned for the production of Cu powder. Al presumably should work too.