Inside a spent laptop battery
I recently acquired an old, and presumably broken (it was in the trash) Macbook Pro Lithium Ion battery. Being the curious fool that I am, I carefully
opened it up to reveal 6 tightly wrapped cells. Upon opening one of the cells I found it was made of a 4 foot long ribbon of what appears to be
aluminum foil coated in a dry black residue. Now according to an outside source, the reaction inside a battery of this type are as follows:
LiCoO2 + C ---> Li1-x CoO2+CLix
But seeing as this battery is permanently dead, I was lead to believe the reaction was messed up, possibly leading to the formation of any of the
following: Li2O, CoO, and CoO2.
My question for anyone that is more tech/electrochemisty-savvy than me, is whether there are some reactions I can carry out to produce lithium and/or
cobalt salts of even a limited purity. As an endnote, I've already immersed some of the ribbon from the battery in water and tried setting it on fire;
neither of them caused any kind of reaction, so it is doubtful that any elemental lithium is present.
[Edited on 22-4-2014 by No Tears Only Dreams Now]
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
If water resulted in no reaction, Li2O can't be present either, so it is likely to be present as LiCoO2 or either of the
products. Not knowing the chemistry of such a curious double salt, I would recommend dissolving in some acid and then adding some base... This might
precipitate Co(OH)2.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Brain&Force
Hazard to Lanthanides
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1302
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline
Mood: Incommensurately modulated
|
|
I highly doubt cobalt dioxide could exist for long. Laptop batteries don't contain lithium metal, either - the technology is different from the
Energizer Lithium batteries. I don't know much about lithium-ion or lithium-polymer batteries.
At the end of the day, simulating atoms doesn't beat working with the real things...
|
|
Zyklon-A
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
Yeah, lithium metal batteries are not rechargeable, only lithium ion batteries are.
|
|