I am looking to make silver nitrate with purity over 99.9%. I don't know much about the processes taken for making reagents of high purity in a lab
and what measures must be taken. I am starting with a silver coin that I have with declared purity of .9999 (4nine pure), I let it sit in 30% HCl for
5 minutes to remove the surface tarnish, and then rinsed well. I make the nitric acid at home by distilling from sulfuric and a nitrate salt inside a
retort and then diluted to 60% with distilled water.
My question is this. The most I have done for cleaning glassware is maybe rinsing with HCl, hot water or ethanol/acetone and then finally rinsing with
distilled water and allowing to air dry. Using pure and clean silver and nitric acid (distilled) my end product should be at least 99.9% pure, using
clean utensils and such, correct?
[Edited on 25-1-2014 by Turner]
|
|
BromicAcid
International Hazard
Posts: 3237
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
99.9% pure by what? Metals?
|
|
Turner
Hazard to Others
Posts: 197
Registered: 2-12-2013
Member Is Offline
Mood: No Mood
|
|
99.9% pure by weight of silver nitrate.
|
|
elementcollector1
International Hazard
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Yes. However, extra steps such as recrystallization couldn't hurt.