Author: Subject: Sodium Sulfide
subsecret
Hazard to Others
***




Posts: 424
Registered: 8-6-2013
Location: NW SC, USA
Member Is Offline

Mood: Human Sadness - Julian Casablancas & the Voidz

[*] posted on 24-7-2013 at 15:22
Sodium Sulfide


I've been needing some sodium sulfide as a testing reagent for lead, as described by TheHomeScientist's channel on YouTube.

Here is the link to the video:
Quote:

http://www.youtube.com/watch?v=SubfXq1rqfM


Would a reaction between sodium sulfate and carbon be sufficient? That reaction is mentioned in this article...

Quote:

http://en.wikipedia.org/wiki/Sodium_sulfide


Thanks, any help is appreciated.




Fear is what you get when caution wasn't enough.
View user's profile View All Posts By User
ParadoxChem126
Hazard to Others
***




Posts: 104
Registered: 5-4-2013
Location: USA
Member Is Offline

Mood: No Mood

[*] posted on 24-7-2013 at 15:25


You can buy it from elemental scientific.
http://www.elementalscientific.net/store/scripts/default.asp




View user's profile Visit user's homepage View All Posts By User
Lambda-Eyde
National Hazard
****




Posts: 860
Registered: 20-11-2008
Location: Norway
Member Is Offline

Mood: Cleaved

[*] posted on 24-7-2013 at 15:43


If you only need it for testing for metals as their sulfides, thioacetamide (if you can find it) also works well.



This just in: 95,5 % of the world population lives outside the USA
Please drop by our IRC channel: #sciencemadness @ irc.efnet.org
View user's profile View All Posts By User
testimento
Hazard to Others
***




Posts: 351
Registered: 10-6-2013
Member Is Offline

Mood: No Mood

[*] posted on 24-7-2013 at 16:04


The carbon reduction of sodium sulfate with carbon requires a high temperature, even up to 900C as per the sodium sulfate melting point, but the method is used in industrial setups with large scale of different sulfates and it works, aside from roasting with hot air to directly dislodge the sulfur dioxide, usually for sulfuric acid prouction scheme. 900C can be reached with ceramic crucible and propane torch using heat shields, but a lot easier way is to use nichrome wire around the crucible with dimmer. Remember to vent the carbon monoxide safely away if you ever procceed to attempt the process.
View user's profile View All Posts By User
subsecret
Hazard to Others
***




Posts: 424
Registered: 8-6-2013
Location: NW SC, USA
Member Is Offline

Mood: Human Sadness - Julian Casablancas & the Voidz

[*] posted on 24-7-2013 at 16:28


Are there any reducing agents that would make the reaction easier to initiate?



Fear is what you get when caution wasn't enough.
View user's profile View All Posts By User
bfesser
Resident Wikipedian
Thread Moved
24-7-2013 at 16:30
gdflp
Super Moderator
*******




Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline

Mood: Staring at code

[*] posted on 21-2-2014 at 11:14


I know this is an old thread, but heating a solution of sodium hydroxide and adding sulfur powder till no more dissolves, then chilling in the freezer to crystallize out the sodium thiosulfate will make sodium sulfide usable for your purposes.
View user's profile View All Posts By User
Zyklon-A
International Hazard
*****




Posts: 1547
Registered: 26-11-2013
Member Is Offline

Mood: Fluorine radical

[*] posted on 21-2-2014 at 12:10


The sodium sulfide wont be anhydrous, though. And it's impossible to separate the hydrates.



View user's profile View All Posts By User
gdflp
Super Moderator
*******




Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline

Mood: Staring at code

[*] posted on 21-2-2014 at 13:06


It doesn't need to be anhydrous for lead testing.
View user's profile View All Posts By User
Zyklon-A
International Hazard
*****




Posts: 1547
Registered: 26-11-2013
Member Is Offline

Mood: Fluorine radical

[*] posted on 21-2-2014 at 13:15


Yeah, it depends on what you need it for.