[*] posted on 25-5-2013 at 05:07
Viton tubing for experiments?


I wanted to use rubber tubing in my experiments for a long time, but fuel, latex, and pvc tubing all become sticky and are essentially destroyed. I wonder if the 20$ for 10 feet of viton tubing wort it. Will it ever corrode?

http://www.aliexpress.com/item/4mm-ID-viton-tubing-resistanc...




I never asked for this.
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 25-5-2013 at 05:33


Quote: Originally posted by plante1999  
Will it ever corrode?
Yes, because everything fails eventually. The right question is whether it lasts long enough to be a more economical choice than the available alternatives. Viton isn't magic, but it resists many things better than the cheaper and more available materials. The ratio of lifetimes and the ratio of costs will tell you whether it's worth it. You may have to acquire a bit of it first and test it for compatibility with whatever you're doing (unstated in your original post).
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 25-5-2013 at 05:47


chlorine, ammonia, sulphur dioxide and all kind of other stuff pass in my tube at around 70 C. Usual rubber is "one use only".



I never asked for this.