hyfalcon
International Hazard
Posts: 1003
Registered: 29-3-2012
Member Is Offline
Mood: No Mood
|
|
Nitric acid/silver nitrate stains
I just had a glove leak today when I was working with my silver purification. My right glove leaked and I didn't realize it at first, now I have
black and brown stained fingers and hand. Is there anything but time that will remove these stains?
|
|
UnintentionalChaos
International Hazard
Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline
Mood: Nucleophilic
|
|
Sandpaper?
Department of Redundancy Department - Now with paperwork!
'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
|
|
kristofvagyok
National Hazard
Posts: 659
Registered: 6-4-2012
Location: Europe
Member Is Offline
Mood: No Mood
|
|
Sandpaper +1.
But be happy, there are several things that can color your hand and looks much worse
I have a blog where I post my pictures from my work: http://labphoto.tumblr.com/
-Pictures from chemistry, check it out(:
"You can’t become a chemist and expect to live forever."
|
|
cyanureeves
National Hazard
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
i am going on a week with stained hands and at least eight of my fingernails blackened by nitric acid. its common for me to go about with one or two
damaged nails but 8 is going to be pretty bad.right now i got my nails covered with white nail polish and it has slowed my nails from cracking all the
way.if the nail polish doesnt work then i will have it pretty bad for a week or so of painful raggety nails as nitric will weaken nails. i have had my
nails crack all the way down passed the middle and have waited until they grew out again,it really sucks because they snag on everything. i just plain
forgot about gloves and i dont even want to know what people think about me when they see my hands.
|
|
hyfalcon
International Hazard
Posts: 1003
Registered: 29-3-2012
Member Is Offline
Mood: No Mood
|
|
Luckily, my solution was pretty loaded down with silver and base metals at the time or it would have been worse. I was only working with ~33% nitric
to begin with and it had been working on 350 grams of sterling for a while.
|
|
kuro96inlaila
Hazard to Self
Posts: 96
Registered: 21-6-2010
Location: Malaysia
Member Is Offline
Mood: Quietly thinking
|
|
I don't think there is other efficient way to remove the stains than time and skinning.
Because the stains it self is reacted keratin.Silver react with keratin to form light sensitive compound and nitric acid nitrated the keratin.
|
|
zed
International Hazard
Posts: 2281
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Nope! We've all had 'em. The stains will be with you until the skin eventually wears off. You will have a nice long time being reminded of your
negligence.
This experience helped me enormously when I was actively playing with chemicals. Made me really cautious about contamination. And thus, even at my
fairly advanced age, I do not have the shakes, the heebie jeebies, or the creeping crawling internal crud we call cancer.
Silver Nitrate contamination on skin, produces a flashy but benign condition, that reminds us of our mortality, and the power of an invisible amount
of a chemical to have a profound effect upon us.
|
|
hyfalcon
International Hazard
Posts: 1003
Registered: 29-3-2012
Member Is Offline
Mood: No Mood
|
|
Had to take the Pediapaw to my own nails instead of the dogs. Sheesh, I'm getting more use out of it then she does.
|
|
cyanureeves
National Hazard
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
one week has passed since i damaged eight of my fingernails and have to say that nail polish has helped a lot.my nails will begain to crack almost
immediately if a chunk of nail polish breaks off and leaves the nail exposed. i think i'm gonna beat this and am starting to love nitric again... and
revlon.
|
|