increasing the surface area of porcelain
I have some smashed porcelain that I am using as boiling chips for boiling sulfuric acid, however there is a problem. No matter how many boiling chips
I add, there is always significant bumping. I suspect this is a problem with surface area, a suspicion that was confirmed when I tried boiling the
sulfuric acid with pumice. When boiling with pumice (which has a huge surface area, much higher than that of boiling chips) no bumping at all was
observed.
However I cannot simply use pumice stones as boiling chips because as my sulfuric acid reaches a certain concentration (around 80-90%) the pumice
starts disintegrating, and the sulfuric acid turns almost opaque with sediment.
The solution as I see it is to increase the surface area of the porcelain by etching it. This can be done with hydrofluoric acid, however a) I don't
have any and b) I don't want to die.
Is there any other way to etch porcelain?
|
|
Vargouille
Hazard to Others
Posts: 380
Registered: 16-4-2012
Member Is Offline
Mood: No Mood
|
|
If you take a piece of coarse sandpaper to it, that might help to increase the surface area. Just be sure to wash it well afterwards.
|
|
hissingnoise
International Hazard
Posts: 3940
Registered: 26-12-2002
Member Is Offline
Mood: Pulverulescent!
|
|
Quote: | No matter how many boiling chips I add, there is always significant bumping. |
Odd? I've never needed chips when heating H2SO4!
That may be because I use a large, shallow casserole dish to concentrate the acid . . .
|
|
chemrox
International Hazard
Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline
Mood: LaGrangian
|
|
Have broken porcelain chips like those worked with other liquids? I don't think the issue is surface area. You may already have too porous a medium.
I think it's more likely a problem with porcelain quality. Some of it may actually be hard baked clay and it disintegrates on heating with strong
acid. If you have a magnetic stirrer that may be the way to go or as hissingnoise says use an open dish. Did you obtain a barrel of battery acid?
"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
|
|
Oscilllator
National Hazard
Posts: 659
Registered: 8-10-2012
Location: The aqueous layer
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by chemrox | Have broken porcelain chips like those worked with other liquids? I don't think the issue is surface area. You may already have too porous a medium.
I think it's more likely a problem with porcelain quality. Some of it may actually be hard baked clay and it disintegrates on heating with strong
acid. If you have a magnetic stirrer that may be the way to go or as hissingnoise says use an open dish. Did you obtain a barrel of battery acid?
|
The broken porcelain chips significantly reduce the bumping, but do not eliminate it. I have not tried the chips on any other liquid apart from water,
where the porcelain chips worked fine.
You seem to have misread my post as you imply that the porcelain disintegrates. It does not, the porcelain does.
I don't have a magnetic stirrer or an open dish, my only borosilicate vessel big enough is a 500ml erlenmeyer flask.