Magnesium Sulphate


If I wanted to create Magnesium Sulphate Anhydrous from Magnesium Sulphate Heptahydrate is there any method of calculating how much heat I would need to drive the excess water off?
View user's profile View All Posts By User
sanity gone
Harmless
*




Posts: 38
Registered: 25-4-2004
Member Is Offline

Mood: No Mood

[*] posted on 25-6-2004 at 00:26


I don't know if that is what you are looking for:
heat = mass x specific heat x temperature change = heat capacity x temperature change
I don't know the specific heat for the dehydration but for water as a gas it is 1.86J/gK
View user's profile View All Posts By User
hodges
National Hazard
****




Posts: 525
Registered: 17-12-2003
Location: Midwest
Member Is Offline


[*] posted on 25-6-2004 at 14:28


I don't know the real answer, but my guess for an estimate would be at least the amount of heat necessary to vaporize the mass of water in question (540 cal/g).
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5126
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 25-6-2004 at 14:34


Do you mean how much heat or do you mean what temperature?
It loses about half of the water if dried at 100C and all the water if you dry it at 300C.
The best way is to keep drying it until it has lost about half its original weight.
View user's profile View All Posts By User
t_Pyro
Hazard to Others
***




Posts: 120
Registered: 7-2-2004
Location: India
Member Is Offline

Mood: Volatile

[*] posted on 25-6-2004 at 20:11


You need to know the enhalpy of hydration of anhydrous magnesium sulfate. If it is "- x" KJ/mole of MgSO<sub>4</sub> with liq. H<sub>2</sub>O, then the heat required to dehydrate y moles of magnesium sulfate is y*x+{heat required to evaporate the water liberated}.