Author: Subject: Preparation of Palladium Acetate from Palladium Chloride
Dope Amine
Harmless
*




Posts: 40
Registered: 29-12-2011
Location: West Coast Baby
Member Is Offline

Mood: No Mood

wink.gif posted on 18-2-2012 at 19:48
Preparation of Palladium Acetate from Palladium Chloride


Any bright ideas on the preparation of palladium acetate from palladium chloride. I'm wondering if stirring a methanolic solution of PdCl2 with sodium acetate would work?

Any help greatly appreciated!
View user's profile View All Posts By User
jon
Hazard to Others
***




Posts: 459
Registered: 11-1-2006
Member Is Offline

Mood: paranoid distrustful apprehensive

[*] posted on 18-2-2012 at 21:22


no i don't think so you would need to make palladium black with formalin and naoh.
then treat it with glacial acetic acid and nitric acid.
note: when you evaporate the acid it can catch fire and sinter i would advise using a vacum.




Give me librium or give me meth!
Patrick Henry....