Acquisition of Methyl Acrylate
Hello! I was wondering if methyl acrylate can be obtained from an OTC source for instance distilling nail polish/super glue or degradation of PMA. I
don't have access to it and would be a fairly useful reagent.
|
|
Dr.Bob
International Hazard
Posts: 2685
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: No Mood
|
|
Methyl acrylate is a noxious, carcinogenic chemical which will polymerize if not kept cold or inhibited with BHT or the like. It is also a potent
sensitizer. It will not be in many retail products as the monomer, being a regulated compound.
You can depolymerize plexiglas to methyl methacrylate (MMA) by careful distillation, but it will repolymerize within a few hours to days, which is
very handy if you want to make a nice clear paperweight with something inside of it. It is also a bit smelly and nasty, but less than MA. This is
a far more useful compound for experiments, due to its ease production and less toxicity.
|
|