[*] posted on 4-3-2004 at 11:21
Immensely stupid question.


I'm not a beginner, but here goes:
What would sulfur trioxide do to a fused
mixture of ammonium phosphate,
magnesium oxide, quarz and crystobalite?

My guess is: nothing. But I want to be sure. I can't find any resistance information w.r.t. SO3 on any of the compounds.

I'm asking because those are the main ingrediants in dental casting mold cement, and I intend to line my catalyst tube on the inside with it (to protect an integral NiCr heating spiral).




My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35

\"Verbing nouns weirds the language!\"
View user's profile View All Posts By User
chemoleo
Biochemicus Energeticus
*****




Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline

Mood: crystalline

[*] posted on 4-3-2004 at 11:32


If the sulphurtrioxide is free of water, I should think that nothing would happen. Best thing is to try - Just put a chunk of your salts into a container and fill that with SO3 (you can get SO3 by heating Na2S2O8 (or 7 even?) by melting it.



Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
View user's profile View All Posts By User
axehandle
Free Radical
*****




Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline

Mood: horny

[*] posted on 4-3-2004 at 11:45


Thanks chemeleo. I was going to use the method of "try and perhaps die" anyway, since I've got more than enough raw materials to build another catalyst chamber should the first one fail. IMHO, I suspect slow erosion, since atmospheric H2O will form sulfuric acid with the SO3 in the chamber.

There is one advantage though: The temperature in the chamber will be 450C, well above the boiling point of H2SO4, so there won't be any H2SO4 floating around in the tube --- it's the gaseous miniscule amount of H2SO4 I'm really worried about.

An idea just struck me: I'll simply pass the ingoing (to the sulfur burner) airstream trough a filter filled with CaCl2. That should kill any pesky H2O molecules.

Science strikes again!




My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35

\"Verbing nouns weirds the language!\"
View user's profile View All Posts By User
t_Pyro
Hazard to Others
***




Posts: 120
Registered: 7-2-2004
Location: India
Member Is Offline

Mood: Volatile

[*] posted on 8-3-2004 at 02:16


My guess would be that magnesium sulfate would be formed. The others won't react for sure. Magnesium oxide is a basic oxide (just below Calcium in the electropositivity series), and hence will react with sulfur trioxide, an acidic oxide.
View user's profile View All Posts By User
axehandle
Free Radical
*****




Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline

Mood: horny

[*] posted on 8-3-2004 at 05:38


Perhaps I'd be better off using gypsum then. It's already thoroughly sulfated, considering it consists of calcium sulfate....

/A