Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Protecting vacuum from H2SO4 vapors?
advanced warning
Harmless
*




Posts: 12
Registered: 6-5-2019
Member Is Offline


[*] posted on 15-11-2022 at 10:44
Protecting vacuum from H2SO4 vapors?


In the interest of exploring flavor compounds, I needed to make food grade sulfuric acid. The hardware store stuff is not acceptable for something I intend to taste.

Using a bath of steel shot and a gas burner, I distilled and collected around 80 mL of clean sulfuric acid. However it was very time consuming and I felt uncomfortable working with 300C+ sulfuric acid.
You would figure that people would vacuum distill it. I'm not really sure why people don't. Before attempting it though, I'd like some input on how to keep my vacuum line safe from H2SO4 vapors.
I'd use a water aspirator, and I have an aluminum check valve, various brass fittings, silicone tubing; all of which would probably have a bad time sucking sulfuric acid. I think this is an actual concern because holding pH paper at the vacuum takeoff (when distilling at atmospheric pressure) shows the air leaving is very acidic.

I was thinking of building a sort of in-line scrubber. Maybe filling a wash bottle with sodium carbonate and pulling a vacuum through that (I don't think I would get very good flow rates, my Na2CO3 is very fine). Or, filling the wash bottle with a saturated solution of Na2CO3 and pulling through that. Maybe hydroxide would be better, I don't know how significant the CO2 production would be.

So, from the vacuum takeoff, into the basic gas wash bottle, then into the vacuum. Maybe there's a concern of boiling the water in the scrubber, I could put it in ice, or bleed off my vacuum if needed.

Does that sound reasonable?
View user's profile View All Posts By User
TLutman
Harmless
*




Posts: 26
Registered: 13-10-2019
Member Is Offline


[*] posted on 15-11-2022 at 14:57


That is what I did. Pick your vactubing wisely. I had 3/8” clear and the heat tends to soften it, letting it collapse.
I have a cold finger that is mounted to the rear of my hood and I just use a beaker with ice and left enough room to add if needed.
View user's profile View All Posts By User
Gammatron
Hazard to Others
***




Posts: 125
Registered: 30-8-2022
Location: Abandoned Uranium Mines
Member Is Offline


[*] posted on 16-11-2022 at 06:20


You can buy PTFE tubing really cheap on eBay, I've used it for distilling HF at over 200C with 0 issues and it can take much more. It's not flexible but it would be suitable to go between your distillation and scrubber and then you can use any type of tubing to go to your pump.



View user's profile Visit user's homepage View All Posts By User
Deathunter88
National Hazard
****




Posts: 519
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline

Mood: No Mood

[*] posted on 16-11-2022 at 08:46


If you are using a water aspirator, all of that is unnecessary. In fact, water aspirators are specifically chosen when corrosive vapors are expected because they get washed out by the stream of water. Besides, aluminum, brass, and silicone are all resistant to sulfuric acid at the concentrations they will come in to contact with.
View user's profile View All Posts By User
advanced warning
Harmless
*




Posts: 12
Registered: 6-5-2019
Member Is Offline


[*] posted on 16-11-2022 at 13:02


Quote: Originally posted by Deathunter88  
If you are using a water aspirator, all of that is unnecessary. In fact, water aspirators are specifically chosen when corrosive vapors are expected because they get washed out by the stream of water. Besides, aluminum, brass, and silicone are all resistant to sulfuric acid at the concentrations they will come in to contact with.


That is a fair point, but part of the reason for asking is to get a new tool for my toolbox which I could use with different reactions, or different setups. I'd be in the same position if I chose to use my nicer pump, for instance.
Or if I'd need to be cognizant of suckback. Intuitively, I don't think suckback should be a problem with H2SO4 because of how low the volatility is, but it might be worth considering when trying to apply the same system to other reactions.
View user's profile View All Posts By User