Colloidal gold from old electronics.


Hello! I made some colloidal gold solution. also very easy to make at home. it needs just acids and old electronics, but very small amounts are necessary. first, I added conc. nitric acid to gold-plated components, as you see not much. then made gold foils and add less than one gram of mercury, when I dissolved it in nitric acid I get this funny amount of gold(PICTURE 2).

IMG-2222.jpg - 1.6MB IMG-2229.jpg - 1.3MB

then I added maybe less than 2ml aqua regia. I diluted the chloroauric acid solution and add carbonate at the same time I was heating it.
The solution got this color (PICTURE 4&5). I did this experiment on a plate because a large area is important. there are some gold particles because I didn't filter it.


IMG-2236.jpg - 2.1MB IMG-2238.jpg - 1.8MB
IMG-2237.jpg - 958kB

[Edited on 6-9-2022 by vano]

[Edited on 6-9-2022 by vano]
View user's profile View All Posts By User
Pumukli
National Hazard
****




Posts: 689
Registered: 2-3-2014
Location: EU
Member Is Offline

Mood: No Mood

[*] posted on 6-9-2022 at 22:06


Looks good.
But why use mercury?
YT is full of "recovering gold from old electronics" videos - but none of them use any mercury... They simply dissolve other metals with nitric acid then dissolve the gold in aqua regia.
View user's profile View All Posts By User
vano
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 6-9-2022 at 22:35


There was very small gold foils particles, polymers waste. So i collect all gold with mercury.