Author: Subject: Epoxy harderner treasure, maybe?
Fantasma4500
International Hazard
*****




Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline

Mood: dangerously practical

[*] posted on 17-4-2022 at 03:09
Epoxy harderner treasure, maybe?


so, visiting some abandoned buildings i came across 10 buckets of some type of epoxy-concrete, and the harderner in plastic bottles right next to it, 5 bottles, some of them almost completely full, 0.66kg each bottle

https://gyazo.com/20f696c5794c60aac1dc26d97cc70226

the contents are rather exotic, amines, some of them compounds that doesnt seem to exist? the contents are:
"Piperatine" - "(Yl?)ethylamine" - "Nonylphenol,3,5,9" - "Triazaundecamethylendiamone" - UN2735 "Polyamines" - "Aminoethylpiperazine"

if i could demolish this molecule into piperazine, which is water soluble i could maybe use that somehow
https://en.wikipedia.org/wiki/Aminoethylpiperazine
https://en.wikipedia.org/wiki/Piperazine

im not quite sure how i would go about seperating these compounds, polyamines is quite a broad term, also includes putriscene. theres a very strong amine smell in the bottle, so there is surely some volatile amines in it, which i could try to first off distill off, or maybe directly react with HCl to form the corresponding salt which would then be water soluble?

i could maybe try to seperate it with heptane fraction from gasoline? any suggestions for what fun i can put this very mixed product through would be interesting, or general ideas for what they can be used for, i have roughly 2 liters of this stuff so i wont let this go to waste.
i did try to find MSDS on it but these bottles are maybe as old as from the 80's, the bathrooms associated with the building where i found the bottles.. there were ashtrays in the bathroom stalls.

i also managed to cash in on about 10kg calcium hypochlorite, 10L 37% H2SO4 and 12kg sodium formate




~25 drops = 1mL @dH2O viscocity - STP
Truth is ever growing - but without context theres barely any such.

https://en.wikipedia.org/wiki/Solubility_table
http://www.trimen.pl/witek/calculators/stezenia.html
View user's profile View All Posts By User