benzil by oxidation of benzoin with NH4NO3 catalyzed by Cu(II) acetate


Reactants:
0,040 g Cu (II) acetate dihydrate (catalyst)
3,72 g benzoin (17,5 mmol) Molar mass 212.24 g/mol https://www.sciencemadness.org/whisper/viewthread.php?tid=68... (I used that second grade crop after using 1,00 g for benzoinoxime https://www.sciencemadness.org/whisper/viewthread.php?tid=15...)
1,9 g NH4NO3
10,0 g acetic acid
2,0 g H2O

All reagents were added into 250 ml reaction flask and reflux condenser attached.

Heated on oil bath, occasionally shaking, N2 bubbles evolution observed already when oil bath 80-110 C, everything dissolved smoothly, then reflux totally for 1,5 h, oil bath temperature 150 C.
(I overkilled the size of the reaction flask, I used 250 ml because I was afraid of gas evolution, but 100 ml flask should be fine, maybe even 50 ml, the evolution of N2 was not vigorous, this could depend on the amount of the catalyst.)

Cooled to room temperature and then to +4 C outside (winter temperature).

Vacuum filtered on sinter, washed with distilled water on sinter, sucked to dryness, air dried for 2 days, last day no more weight decreasing observed.

Yield 3,35 g = 15,9 mmol (91%) of nice yellowish crystals. Molar mass 210.232 g·mol−1.

m.p. 95,0-96,0 C (lit. 94.0 to 96.0 °C https://en.wikipedia.org/wiki/Benzil)

some further experiments starting from benzil (phenytoin, benzilic acid rearrangement, benzil dioxime = Ni(II) indicator)
https://www.sciencemadness.org/whisper/viewthread.php?tid=15...
https://www.sciencemadness.org/whisper/viewthread.php?tid=19...
https://www.sciencemadness.org/whisper/viewthread.php?tid=19...


Attachment: vogel_benzil.pdf (136kB)
This file has been downloaded 186 times



reagents from the left: copper (II) acetate dihydrate, benzoin, NH4NO3, acetic acid

IMG_20211205_142504_6.jpg - 50kB



after adding everything into reaction flask (smaller flask should be used, N2 evolution slow enough)

IMG_20211205_143028_9.jpg - 16kB



after reflux

IMG_20211205_164354_9.jpg - 26kB



after cooling down to +4C

IMG_20211205_171610_8.jpg - 29kB



vacuum filtered on sinter

IMG_20211205_201245_0.jpg - 18kB



nice pale yellow crystals of the product (I like such synthesis where recrystallization not necessary, here the crystallization happened directly from the reaction mixture, according Vogel recrystallization does not change m.p., the product is already pure enough)

IMG_20211207_144648_6.jpg - 70kB

[Edited on 7-12-2021 by Fery]




View user's profile Visit user's homepage View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1225
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 10-12-2021 at 22:16


Hi, Fery, very nice description! Do you have some plans with your benzil?



View user's profile View All Posts By User
karlos³
International Hazard
*****




Posts: 1520
Registered: 10-1-2011
Location: yes!
Member Is Offline

Mood: oxazolidinic 8)

[*] posted on 10-12-2021 at 23:29


Uh thats nice and surprisingly simple, while I also still have lots of benzoin.

The benzil even has the nice neon-greenish colour as a liquid I know from other alpha-diketones like 1-phenyl-1,2-propanedione and 1-phenyl-1,2-hexanedione.

Are you going to aminate it, for ephenamine for example?
Alpha-diketones are really nice to make 1,2-aminoalcohols from via reductive amination, they will selectively aminate only on one carbonyl.

[Edited on 11-12-2021 by karlos³]




verrückt und wissenschaftlich
View user's profile View All Posts By User
Fery
International Hazard
*****




Posts: 1000
Registered: 27-8-2019
Location: Czechoslovakia
Member Is Offline


[*] posted on 11-12-2021 at 03:17


Hi Bedlasky and karlos³
these 3:
phenytoin (reaction with urea)
benzilic acid (rearrangement with alkaline hydroxide)
diphenylglyoxime (reaction with 2 moles hydroxylamine) this is Niclon indicator, analogue of dimethylglyoxime, it does not have any advantage over commonly used dimethylglyoxime, I just want to see its color with Ni(II)
Boffis if you are reading this, you can try the same with the 2,2'-furoin and 2,2'-pyridoin you synthesized (the first link in my first post).




View user's profile Visit user's homepage View All Posts By User
Boffis
International Hazard
*****




Posts: 1843
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 11-12-2021 at 09:16


Hi Fery, Nice work and a good write-up.

I have run this reaction myself but never seem to have posted it. It works well with Benzoin, reasonably with furoin but fails with pyridoin.

I tried nitric acid on pyridoin as in Vogels procedure for the nitric acid oxidation of benzoin to benzil but the reach is very vigorous and difficult to control. More dilute nitric acid may work better as when the first ml or so of nitric acid is added a yellow product is formed that later dissolves. When only half the nitric acid has been added oxidation appears complete and every thing dissolve. Neutralisation ppt only a little red powder.