Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Using silver shot for a heat bath instead of sand?
RogueRose
International Hazard
*****




Posts: 1593
Registered: 16-6-2014
Member Is Offline


[*] posted on 6-5-2021 at 08:47
Using silver shot for a heat bath instead of sand?


I was just looking at some posts about using a sand bath for some distillations (including H2SO4) and I was wondering if something like pure silver shot would be a better choice (if it's already available - I know it's expensive for what it is...). I was amazed at how fast a 1oz silver round melted an ice cube I set on top of it - it was amazingly fast for the coin only being heated by my hand before putting the ice cube on it. I know it's only a little more thermally conductive than copper (I've seen sources say 9%) but it seems much higher for some reason.

View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4581
Registered: 11-1-2014
Location: Salt Lake City
Member Is Online

Mood: PhD candidate!

[*] posted on 6-5-2021 at 09:06


Copper or aluminum shot is already well known as an excellent heating medium. Presumably silver would work just as well if not marginally better, though as you point out, it would be prohibitively expensive for that use, so you may as well compromise and use copper.