Ended up with several of these gaskets. Assumed they were lead they are quite thin.
Crushed one up and hit it with a propane flame, took to red heat...no change ..as you can see in the photo.
Any ideas? I dont think i can measure the volume accurately so getting a density is out.

20201211_200749.jpg - 1.5MB
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1694
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 11-12-2020 at 08:41


Maybe it is some form of flexible graphite, possibly metal reinforced.
https://mtigasket.com/metal-reinforced-gasket-materials/cors...
https://www.indiamart.com/proddetail/flexible-graphite-gaske...
http://www.bestsealing.com/sale-9283817-graphite-gasket-rein...

[Edited on 11-12-2020 by Morgan]