Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Nickel Chloride Crystallization
artemov
Hazard to Others
***




Posts: 181
Registered: 22-8-2018
Member Is Offline


[*] posted on 24-11-2020 at 06:47
Nickel Chloride Crystallization


I made some nickel chloride solution (using pure nickel coins, H2O2 and HCl) from which I am trying to get the hexahydrate crystals via slow evaporation in open air.

Unfortunately I just found out that "the nickel chlorides are deliquescent, absorbing moisture from the air to form a solution" (https://en.wikipedia.org/wiki/Nickel(II)_chloride)

Can a hygroscopic salt crystallized via slow evaporation in the open air? If not, what can I do besides heating/boiling the solution, something I am reluctant to do? Cheers.
View user's profile View All Posts By User
CarlSagans_RayGuns
Harmless
*




Posts: 14
Registered: 9-4-2018
Member Is Offline

Mood: No Mood

[*] posted on 24-11-2020 at 07:07


Have you tried putting it in a sealed bag with magnesium sulfate desiccant? You might still need a little bit of heat. I dry mine in open air over a heating pad. Wear a respirator and nitrile gloves, no biggie. You want to avoid breathing the dust.
View user's profile View All Posts By User
Tsjerk
International Hazard
*****




Posts: 3032
Registered: 20-4-2005
Location: Netherlands
Member Is Offline

Mood: Mood

[*] posted on 24-11-2020 at 07:22


Hygroscopic salts can only be dried in open air when the relative humidity is below a certain threshold. In a closed container with for example magnesium sulfate or calcium chloride you will bring down the humidity so far, the salt will dry. Under vacuum the salt dries faster, but with a little patience any closed container will do.
View user's profile View All Posts By User
MidLifeChemist
Hazard to Others
***




Posts: 192
Registered: 4-7-2019
Location: West Coast USA
Member Is Offline

Mood: precipitatory

[*] posted on 24-11-2020 at 08:05


>> If not, what can I do besides heating/boiling the solution, something I am reluctant to do?

Is it because you are worried about the quality of the crystals, or some other reason?
View user's profile View All Posts By User
artemov
Hazard to Others
***




Posts: 181
Registered: 22-8-2018
Member Is Offline


[*] posted on 24-11-2020 at 08:06


There is still a lot of water currently. I think I will wait for the water/hcl to reduce by a fair amount first before doing the dessicating box thing. Thanks guy!

MidLifeChemist: for safety reason

[Edited on 24-11-2020 by artemov]
View user's profile View All Posts By User

  Go To Top