Author: Subject: NO2 ventilation in HNO3 distillation
Zinc
Hazard to Others
***




Posts: 472
Registered: 10-5-2006
Member Is Offline

Mood: No Mood

[*] posted on 26-2-2011 at 10:45


Today I tried to distill HNO3 from a distillation flask closed by a plastic cork (I don't know what kind of plastic) wrapped in 5 layers of Al foil. The Al foil was not dissolved by nitric acid and sucessfuly protected the cork.