Author: Subject: Grow Calcite Crystals and Birefringence
Sivvy
Harmless
*




Posts: 6
Registered: 1-7-2017
Member Is Offline

Mood: No Mood

[*] posted on 26-11-2019 at 18:09
Grow Calcite Crystals and Birefringence


Does anybody have any information regarding growth of calcite crystals? I want to grow a clear calcite crystal and observe birefringence through it (as seen with the calcite crystal here: https://en.wikipedia.org/wiki/Birefringence).

I haven't found any good information on growing such a crystal, as all the information for growing calcium carbonate crystals relates to growing aragonite, which is beautiful, but not what I am after.

Thanks for any help or leads!
View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1308
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 26-11-2019 at 20:00


https://www.jstage.jst.go.jp/article/jcersj1988/101/1169/101...

Not exactly simple.




Helicopter: "helico" -> spiral, "pter" -> with wings
View user's profile View All Posts By User
Sivvy
Harmless
*




Posts: 6
Registered: 1-7-2017
Member Is Offline

Mood: No Mood

[*] posted on 26-11-2019 at 20:38


What keywords and search engine did you use to find that paper?
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 27-11-2019 at 01:13


Sodium nitrate is isostructural with calcite, birefringent and much easier to crystallise
View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1308
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 27-11-2019 at 13:35


Quote: Originally posted by Sivvy  
What keywords and search engine did you use to find that paper?


I think I just used "calcite crystal growing hydrothermal". On google. There are a few papers out there, but mostly behind paywalls.

[Edited on 27-11-2019 by Twospoons]




Helicopter: "helico" -> spiral, "pter" -> with wings
View user's profile View All Posts By User
Sivvy
Harmless
*




Posts: 6
Registered: 1-7-2017
Member Is Offline

Mood: No Mood

[*] posted on 27-11-2019 at 15:30


Quote: Originally posted by unionised  
Sodium nitrate is isostructural with calcite, birefringent and much easier to crystallise


In the paper that Twospoons linked to, they dissolved the calcium carbonate in ammonium nitrate, noting that the nitrate ion is isostructural, making it a good solvent of calcium carbonate. That fascinates me.

I'm going to look into sodium nitrate crystallization now. I appreciate the redirection on that.
View user's profile View All Posts By User
rockyit98
Hazard to Others
***




Posts: 283
Registered: 12-4-2019
Location: The Known Universe
Member Is Offline

Mood: no mood is a good mood

[*] posted on 27-11-2019 at 15:45


in nature they form from calcium bicarbonate.maybe you can dissolve CaCO3 in pressurized CO2 and slowly let gas out to make big crystals.



"A mind is a terrible thing to lose"-Meisner
View user's profile View All Posts By User
Sivvy
Harmless
*




Posts: 6
Registered: 1-7-2017
Member Is Offline

Mood: No Mood

[*] posted on 2-12-2019 at 11:26


Crystallizing them in pressurized CO2 definitely sounds like a fascinating project, but it is currently beyond my means.
View user's profile View All Posts By User
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 2-12-2019 at 12:56


https://en.crystalls.info/Sodium_nitrate
It has a photo demonstrating NaNO3's birefringence.




View user's profile View All Posts By User
Tsjerk
International Hazard
*****




Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline

Mood: Mood

[*] posted on 2-12-2019 at 14:36


Try to grow a triglycine disulfate crystal. I got a three centimeter crystal easily, I just left the solution to evaporate at room temperature and normal pressure. The birefringence was obviouse.

I found the crystal after holidays and there was a void in the crystal where it was on the bottom of the beaker, so lifting the growing crystal from the bottom is probably a good idea.

Edit: oops, it was triglycine sulfate, not disulfate

[Edited on 3-12-2019 by Tsjerk]