porous plate
I occaisionally see a "porous plate" specified in a procedure, especially in some of the older ones. It's usually used for drying wet crystals.
I don't know exactly how these are made but I'm thinking that one could easily be made with a potter's wheel and then fired in a kiln. I'm thinking
that a mix of 50% kaolin clay, 25% feldspar, and 25% SiO2 would make a nice white plate. I don't know what would be the best proportions for the
right porosity. Any suggestions?
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
You've got the idea, just about any general purpose clay works and fireclays were common. Also for those without facilities for making their own,
pottery supply shops often carry unfired greenware, bisqued, or fully fired plain unglazed tiles such as http://www.dogwoodceramics.com/Products/unglazed_ceramic_bis...
I'd just wedge the clay then roll it out, with an old rolling pin if nothing else.
The optimal pore size varies some with the product crystal size and shape, but doesn't seem to be too critical.
|
|
Sedit
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1939
Registered: 23-11-2008
Member Is Offline
Mood: Manic Expressive
|
|
I have a ton of these since I have a kiln and much experience in ceramic works. Honestly, I love them. There are times where they shorten a process so
much that I couldn't live without them. My suggestion since its for chemical work is to just go with Porcelain since its some of the highest quality
clay around and its pore structure is quite small while still allowing substances to dry quickly.
Take care to only fire the clay to bisqe ware temperatures to avoid vitrification else all your work would be in vain and you would have nothing more
but a piece of glass.
Knowledge is useless to useless people...
"I see a lot of patterns in our behavior as a nation that parallel a lot of other historical processes. The fall of Rome, the fall of Germany — the
fall of the ruling country, the people who think they can do whatever they want without anybody else's consent. I've seen this story
before."~Maynard James Keenan
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
Thanks to both of you for the good suggestions. And Sedit, I'm glad to see that somebody is actually putting porous plates to good use.
I do think I will investigate what my local pottery shop has for bisqueware before trying to make one of my own.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|