Dr. N Butyl Lithium makes a phosphorescent powder from microwave combustion synthesis using:

Watch: http://www.youtube.com/watch?v=TYDn06G2C0E

1.875g of Aluminum Nitrate Nonahydrate
530mg Strontium Nitrate
10.7mg Europium Nitrate Pentahydrate
21.9mg Dysprosium Nitrate Pentahydrate
30.9mg Boric Acid

3mL distilled water is used as the solvent.

3.9g of Urea is added to that mixture and it is shaken until fully dissolved.

It can be ignited in a vile by torch but this yields lower quality product.

It is ignited by placing the vile in a beaker and microwaving. This ignites the mixture.

My question. What products are formed? And what reactions are taking place during the combustion.




View user's profile Visit user's homepage View All Posts By User
Picric-A
National Hazard
****




Posts: 796
Registered: 1-5-2008
Location: England
Member Is Offline

Mood: Fuming

[*] posted on 12-6-2010 at 01:22


The product is mostly Aluminium oxide, doped with Strontium, Europium and Dysprosium oxide with a trace of boric oxide to act as a light intensifier.

I am unsure as to the purpose of the urea however.
View user's profile View All Posts By User This user has MSN Messenger
The_Davster
A pnictogen
*******




Posts: 2861
Registered: 18-11-2003
Member Is Offline

Mood: .

[*] posted on 12-6-2010 at 04:15


Rare earth-doped strontium aluminate.
I have prepared this by sol-gel synthesis and then calcining, but this procedure seems far easier. I think urea is the solvent (at high T once water is driven off) and microwave absorber in this case, but I could be wrong.

Your nitrates are calcined to the corresponding oxides. Under the high temperatures the strontium aluminate structure is formed.




View user's profile View All Posts By User
Vogelzang
Banned





Posts: 662
Registered: 26-4-2008
Member Is Offline

Mood: No Mood

[*] posted on 12-6-2010 at 06:22


Ultra Green powder. I think its doped Strontium Aluminate.
http://www.4shared.com/video/SwsjOVD5/Luminescent.html

http://shop.ebay.com/i.html?_nkw=ultra+green+powder&_sac...



[Edited on 12-6-2010 by Vogelzang]
View user's profile View All Posts By User
not_important
International Hazard
*****




Posts: 3873
Registered: 21-7-2006
Member Is Offline

Mood: No Mood

[*] posted on 12-6-2010 at 09:53


Vogelzang has it. The urea functions as a reducing agent to form Eu(II), and as a fuel to generate additional heat. Boric oxide functions as a flux.

Lotta stuff about it on da web

Microwave Synthesis of a Long-Lasting Phosphor
http://pubs.acs.org/doi/abs/10.1021/ed086p72



Attachment: jpconf9_187_012017.pdf (773kB)
This file has been downloaded 943 times

Attachment: dis1.7.pdf (331kB)
This file has been downloaded 1321 times

Attachment: 0405110.pdf (635kB)
This file has been downloaded 700 times
View user's profile View All Posts By User

  Go To Top