Daniel
Harmless
Posts: 1
Registered: 18-1-2004
Member Is Offline
Mood: No Mood
|
|
Ionising Cu, Zn
Please help, I need to ionize Cu and Zn with acid?
|
|
Saerynide
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
Cu disolves in hot H2SO4. I think Zn probably does too, not sure about that though.
You could also electrolyze them by using a copper or zinc anode and a stainless steel or carbon cathode. Use an electrolytic solution of magnesium
sulfate. Check the Copper Sulpate thread in Electrochemistry.
|
|