Platinum Indium alloy


While trying to show the gorgeous color of indium in the flame to a friend of mine, I put a small piece of In metal on a Pt wire. The indium melted quickly in the flame, but at red hot temperature it started to dissolve the Pt wire, turning into a slightly larger and much harder blob of metal that advanced along the wire, consuming it.

This reaction seems to be of the "bimetalic fuse" kind (Pt/Al wire I guess) a member (Axt) documented.

Moral of the story: never use metals but salts for watching the flame colors on Pt wire.

Pics later.
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 28-12-2009 at 00:26


Ah yes, all kinds of things attack platinum. It's really pretty awful as "inert" substrates go!

Let's see, In-Pt... there's a phase diagram, but it only goes up to 30%at! Only enough to show the first intermetallic, InPt3. Well, if Pt-Sn is representative, there's probably a series of brittle intermetallics of descending melting point, all the way down to In, with the liquidus line being roughly diagonal, so you might get 25% Pt in solution at somewhat more than 25% of the way between the melting points (1000K or so?).

It's probably not very exothermic as reactions go (not like nickel + aluminum), but it will certainly proceed.

Tim

[Edited on 12-28-2009 by 12AX7]




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger

  Go To Top