Uranium carbonate leach next steps?
Hi,
i have successfully leached uranium ore using sodium bicarbonate. It glows green under blacklight. My question is, how can i further process the
solution. I assume that i should boil it down, but im not sure how to get it to uranium peroxide. I cant find anything about the process and would
like some guidance on where i can find documentation, if there is any.
Thanks,
Jackson
|
|
phlogiston
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1377
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
Have you seen Carl Willis page?
https://carlwillis.wordpress.com/2008/02/20/uranium-chemistr...
Briefly: adjust the pH with acid to the right range and add peroxide.
-----