chemical glass
I have been buying glassware made out of Borosilicate. Is it the same as Pyrex?Or is one better then the other if its not? Can there be drawbacks to
one type of class over another? thank you for any help. Beastmaster
|
|
bfesser
Resident Wikipedian
Posts: 2114
Registered: 29-1-2008
Member Is Offline
Mood: No Mood
|
|
For all practical purposes, it's the same thing. Pyrex is just Corning's name for their borosilicate glassware.
|
|
Picric-A
National Hazard
Posts: 796
Registered: 1-5-2008
Location: England
Member Is Offline
Mood: Fuming
|
|
Pyrex glassware is borrosilicate i believe but better made so it is resistant to cracking due to sudden changes of heat. Pyrex is definitly one of the
best you can buy, but it is much more expensive.
You can buy cheap borrosilicate glassware under different brand names (Bomex, Simex ect..) but there are theads on these and which to choose.
|
|