Sciencemadness Discussion Board

Ba(NO3)2 - NaNO3 - eutektikum (temperature ?)

chief - 16-9-2007 at 06:37

What is the temperature of Ba(NO3)2 - NaNO3 - eutektikum (if it exists, since the compounds should at least at some temperatures/compositions be immiscible) ?

Jamjar - 16-9-2007 at 07:09

Searching for NaNO3 at the Molten Salt Database -Eutectic Finder then finding Ba(NO3)2 within the results...

System, Composition (mol percent), Eutectic Temp.
Ba(NO3)2-NaNO3, 6.4-93.6, 294 C
Ba(NO3)2-NaNO3, 5.8-94.2, 295 C
Ba(NO3)2-NaNO3, 6.4-93.6, 298 C

DerAlte - 16-9-2007 at 21:00

@Jamjar - Useful reference! Thanks, Der Alte

chief - 17-9-2007 at 06:04

Are there more useful databases ? Any overview ?
If anyone needs crystal-structures (inorganic), I can provide them .