If it is not quartz, it could make a nice starting point for large ampoules of chlorine, bromine etc. for an element collection.
If its quartz you can cut it but you won't be able to fuse it or bend it without an oxygen/propane torch or similar. That's another way to test for
quartz btw: if it looks like glass but you can't melt it, then its probably quartz. |