I buy most of my glass from Chinese sellers on eBay but when I can afford to pay the extra money I will order Laboy glass. The problem with Chinese
sellers is the time it takes to receive the product and sometimes the quality. Laboy glass is great as it is not as expensive as say chemglass or
Pyrex and is also of good quality.
I'm looking for other sellers such as Laboy or even lower quality glass but shipped from within the US so I don't have such long wait times. Does any
one here have any reliable sellers from within the US they could point me to?
Also I have a couple end flasks with the logo "labuddy" which are of great quality and I bought them thinking they were Laboy but when I go to search
the term labuddy on eBay I can't find anything. Does any one have info on this seller? Abromination - 28-7-2018 at 15:41
Cheap? Not pyrex, then.
Or any other primary laboratory glassware manufacturer. If you were in the US I would suggest Karter Scientific, but they charge 15 USD for shipping.zed - 6-8-2018 at 16:16
Deschem shipments (from China) often arrive within 7 days. At least, in Portland.
Depends. happyfooddance - 6-8-2018 at 18:20
I know that if you order glass from Laboy from Amazon, rather than their website, they are MUCH more prompt an punctual. It still takes the same time
to ship (about a week to CA), but it gets shipped a day or two after the order is placed, IME. I think this might be because they don't stock
everything listed on their site, but the stuff on Amazon is already made and ready to ship. For what it's worth.ELRIC - 7-8-2018 at 03:38