TheBlackPope - 1-6-2007 at 07:11
In what kind of stores may one find this OTC?
garage chemist - 1-6-2007 at 07:21
None.
Cyclohexanone is however easily made from adipic acid, which can be bought cheaply as a food additive (though not OTC).
[Edited on 1-6-2007 by garage chemist]
Maya - 1-6-2007 at 13:23
usual ingredient in PVC cement
garage chemist - 1-6-2007 at 23:33
Oops, I confused it with cyclopentanone, which isnt OTC. My bad.
Cyclohexanone is found in PVC cement, in admixture with other solvents like THF. Fractional distillation can be used to separate pure cyclohexanone.
jackson2004 - 24-6-2007 at 19:18
I can get Cyclohexanone and others similar quite cheaply.
I also have a Cyclohexanol supplier but they are situated in the US ( I am in the uk )
PM me if you are looking to buy some or trade for some of either and i will contact my chem supplier and see what i can do.
Also please contact me if you have any chemicals and are looking to trade / sell some.
The last purchase of Cyclohexanone i payed about £8 including postage for 250ml.
[Edited on 24-6-2007 by jackson2004]
Drunkguy - 24-6-2007 at 23:23
why dont u just buy more then. thats not a bad price for a PI (private individual).
jackson2004 - 25-6-2007 at 01:59
If Drunkguy was talking to me, it because its not me that is wanting the chemical. I was just stating the price i pay. If i wanted more i would buy
more, i know its not a bad price.
[Edited on 25-6-2007 by jackson2004]
dedalus - 25-6-2007 at 03:22
You could look at Hach's website, for cyclohexanone. They sell 100 ml bottles in conjunction with their "Zincon" method for Zn analysis in wastewater.
https://www.hach.com/
Not cheap, perhaps. But they're easy to do business with.
[Edited on 25-6-2007 by dedalus]
[Edited on 25-6-2007 by dedalus]
jackson2004 - 25-6-2007 at 10:02
Speak to me if in the uk and i will provide an email for a supplier 250ml for £8 if you are in the uk.
Prob 1l for £25 or so