I would convert it to KClO3. Just dissolve all of it in as little as possible of water, allow insoluble stuff to settle and then mix the clear
solution with a concentrated solution of KCl. If white solid appears, then boil, until everything is dissolved again, and then slowly allow to cool
down.
From the remaining liquid you can get more KClO3 by boiling it down and then letting it cool down again. |