TiO2 sounds about right.
TiCl3 is not stable in aqueous solution and even in strong solutions of HCl it will hydrolyse over a matter of days if not hours.
OTOH, TiO2 is pretty impervious to HCl and will sit happily, doing nothing in the bottom of a container. |